The depfeted and enriched regions of solute atoms formed by spinodal decomposition in the early stage of tempering for ultrahigh strength steel 23Co14Ni12Cr3 we
The tungsten alloys with Ni-Cu and Fe-Cu additives were sintered at 1573 K for 1 h by hot-pressing method. It was found that the alloy relative density can be i