论文部分内容阅读
SiC/7075 aluminum matrix composites were prepared by a liquid stirring method. The role of Ti facilitating the preparation of SiC/7075 aluminum matrix were studied by means of direct-reading spectrometer, scanning electron microscope, energy dispersive spectrometer, X-ray diffraction and the sessile drop method. The results show that the SiC content in the SiC/7075 composite increases with an increase of Ti addition. The addition of Ti can significantly improve the wettability of SiC/Al system, there is a critical value of above 0.5% of Ti content in improving the wettability of the Al/SiC system at 1173 K. The temperature of the “non wetting-wetting” transition for the (Al-2Ti)/ SiC system is about 1123 K, the contact angle decreases to 88 ° at 200 seconds and reaches a stable contact angle of 28 ° at 2100 seconds.