Mechanism of mechanical activation for sulfide ores

来源 :中国有色金属学会会刊 | 被引量 : 0次 | 上传用户:wuxinghui_1975
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
Structural changes for mechanically activated pyrite, sphalerite, galena and molybdenite with or without the exposure to ambient air, were systematically investigated using X-ray diffraction analysis(XRD), particle size analysis, gravimetrical method, X-ray photo-electron spectroscopy(XPS) and scanning electron microscopy(SEM), respectively. Based on the above structural changes for mechanically activated sulfide ores and related reports by other researchers, several qualitative rules of the mechanisms and the effects of mechanical activation for sulfide ores are obtained. For brittle sulfide ores with thermal instability, and incomplete cleavage plane or extremely incomplete cleavage plane, the mechanism of mechanical activation is that a great amount of surface reactive sites are formed during their mechanical activation. The effects of mechanical activation are apparent. For brittle sulfide ores with thermal instability, and complete cleavage plane, the mechanism of mechanical activation is that a great amount of surface reactive sites are formed, and lattice deformation happens during their mechanical activation. The effects of mechanical activation are apparent. For brittle sulfide ores with excellent thermal stability, and complete cleavage plane, the mechanism of mechanical activation is that lattice deformation happens during their mechanical activation. The effects of mechanical activation are apparent. For sulfide ores with high toughness, good thermal stability and very excellent complete cleavage plane, the mechanism of mechanical activation is that lattice deformation happens during their mechanical activation, but the lattice deformation ratio is very small. The effects of mechanical activation are worst.
其他文献
By using the spark plasma sintering process, Ti2AlC/TiAl composite with the addition of Niobium (Nb) was prepared in-situ and the microstructure of Ti2AlC/TiAl
Isothermal and cyclic oxidation behaviors of chromium samples with and without nanometric CeO2 coating were studied at 900 ℃ in air. Scanning electron microsco
CdGd2(WO4)4-δ single crystal was grown using the Czochralskis method. The crystal structure was tetragonal scheelite with lattice parameters a=b=0.5203 nm and
Ceramic microspheres were prepared by using Chinese bauxite as raw materials through the centrifugal spray drying method. The control technology of microsphere
Ni-W-P-CeO2-SiO2 nano-composite coatings were prepared on the carbon steel surface by pulse co-deposition of nickel, tungsten, phosphorus, nano-CeO2 and nano-Si
Investigation into the magnets with different squareness of hysteresis loop (SHL) reveals that the microstructure of sintered NdFeB magnets has great effects on
A novel method was applied to the surface modification of the metal hydride(MH) electrode of MH/Ni batteries. Both sides of the electrode were plated with a thi
Conducting blends of polyacrylonitrile (PAN) copolymer and dodecylbenzene sulfonic acid doped polyaniline (PANI-DBSA) were prepared by solution blending of the
Hollow spheres of hexagonal ferrite BaCo2Fe16O27 were fabricated through a spray pyrolysis technique using co-precipitation ferrite powder precursor as material
The production of MoO_3 from Sarcheshmeh molybdenite concentrate via a pyro-hydrometallurgical process was studied.The molybdenite concentrate and sodium carbon