论文部分内容阅读
摘要:为了保证人们对住宅工程高质量的要求,我们在住宅工程施工过程中,严格要求,按照规范标准进行操作,并加强管理,尽可能的加强对这些质量通病的预防和处理,住宅工程的质量通病还是可以消除或避免的。本文主要针对目前建筑工程施工中,住宅工程中一些常见的质量通病与防治技术进行了全面的探讨。
关键词:质量通病;危害性;原因分析;治理技术;要点;重视
Abstract: In order to ensure that people of residential engineering quality requirements, we in the housing project construction process, strict requirements, in accordance with the standards of operation, and to strengthen the management, as far as possible, to strengthen the quality defects prevention and treatment, residential project quality common fault can be eliminated or avoided. This article mainly aims at the present building construction, residential projects in some of the common quality fault and prevention technology to conduct a comprehensive study.
Key words: quality; harm; cause analysis; control technology; key points; attention
中圖分类号:TU71献标识码: A 文章编号:2095-2104(2012)12-0020-02
1.住宅工程质量的危害性及防治对策
随着我国住宅基本政策和制度由公有化福利型向商品化市场型转变,使得与住宅的建设、质量、维修等有关法律维权的人也越来越多。老百姓用一辈子的积蓄买上一套商品住宅不容易,所以对居住环境和住宅质量的要求不断提高,为了提高住宅工程质量,满足住户对住宅工程质量不断完善的预期,住宅工程的质量是“百年大计”,与人民生命财产休戚相关。近年来,住宅工程质量通病导致的影响主体结构安全和影响使用功能已成为引起住户投诉的焦点,所以作为设计单位、建设单位、监理单位、施工单位各方的专业技术管理人员必须重视住宅工程质量,尤其是施工单位项目负责人和工程技术人员,掌握治理住宅质量通病的技巧,住宅工程质量一定会得到大大提升。
2.水泥地面起砂和空鼓的治理
2.1材料因素
2.1.1使用了水泥标号低或水泥受潮而降低了水泥强度等度的水泥。
2.1.2砂子含泥量大,颗粒过细,造成水灰比加大,强度降低。
2.2施工原因及防治
2.2.1使用强度不低于42.5级水泥,砂子采用中砂,细度模数为2.3~3.0。
2.2.2没有掌握压光时间和压光遍数;由于不掌握水泥硬化的机理,压光过早,水泥凝胶未形成,游离水过多,压光只是形成水光,其强度和抗磨能力不好;水泥终凝后再压光,操作困难并影响已硬化的表面,大大降低面层的强度和抗磨能力;水泥地面压光应在水泥终凝前,压光遍数一遍为2~3遍。
2.2.3水灰比大,砂浆强度降低容易造成起砂,控制好砂浆稠度。
2.2.4冬期施工砂浆受冻,强度降级容易造成起砂。
2.2.5养护不当,未到24h就浇水或地面缺水影响水泥的水化作用;养护时间不到就上人走动或进行下道工序的施工,造成地面的破坏和起砂。
2.2.6基层表面未清理干净,有浮灰和其它污物,影响与基层结合粘接,造成空鼓。
2.2.7垫层基层表面有积水也影响面层与基层的粘接力,造成空鼓。
2.2.8基层润湿不够,刷浆过早,造成风干硬结而形成隔离层。刷浆不均匀,存在干灰点也容易空鼓。
2.2.9砂浆层过薄,养护不及时,造成失水过快,影响与基层粘接造成空鼓,造成收缩干裂空鼓。
3.砌体裂缝和渗漏的治理
由于建筑物墙体裂缝、渗漏涉及的纠纷或官司越来越多,建筑物墙体裂缝已成为住户评判建筑物安全的一个非常直观、敏感和首要的质量标准。
3.1原因分析
引起砌体结构墙体裂缝的因素很多,既有地基、温度、干缩,也有设计上的疏忽、施工质量、材料不合格及缺乏施工经验等。
3.2砌体裂缝的种类
3.2.1八字型裂缝:
当外界温度上升时,外纵墙本身沿长度方向将有所伸长,但屋盖部分的伸长量比墙体的伸长量大得多,从而对墙体产生附加水平推力,墙体受到屋盖的推力而产生剪应力,剪应力和拉力又引起主拉应力。当主拉应力过大时,将在墙体上产生八字型裂缝,如在门窗洞边的八字型裂缝。
3.2.2水平裂缝和包角裂缝:
由于屋面伸长或缩短引起的向外或向内的推力产生的屋面板部或顶层圈梁下沿砖(砌块)灰缝的水平裂缝和砼平屋盖房屋顶层两端的墙体上包角裂缝。
3.2.3女儿墙裂缝:
由于屋面板和水泥砂浆面层发生过大温度变形,使女儿墙根部受到向外或向内的水平作用力而引起的女儿墙根部与平屋面交接处砌体外凸或女儿墙外倾所产生的裂缝。
3.2.4垂直裂缝:
当房屋的楼(屋)面为现浇钢筋混凝土结构时,由于收缩和降温引起的楼(屋)面缩短受到了墙体的限制,使楼(屋)面构件处于受拉状态。如果房屋过长,或设计时按采暖考虑而实际上未采暖,则可能在楼(屋)面上每隔一定距离发生贯通全宽的裂缝,在四个角发生八字型裂缝。当房屋有错层时,错层处的墙体容易产生局部的垂直裂缝。
3.2.5干缩裂缝:
烧结粘土砖,包括其它材料的烧结制品,其干缩变形很小,且变形完成比较快。只要不使用新出窑的砖,一般不要考虑砌体本身的干缩变形引起的附加应力。但对这类砌体在潮湿情况下会产生较大的湿胀,而且这种湿胀是不可逆的变形。对于砌块、灰砂砖、粉煤灰砖等砌体,随着含水量的降低,材料会产生较大的干缩变形,但是干缩后的材料受湿后仍会发生膨胀,脱水后材料会再次发生干缩变形,但其干缩率有所减小,约为第一次的80%左右。这类干缩变形引起的裂缝在建筑上分布广、数量多、裂缝的程度也比较严重。
3.3砌体裂缝的控制措施
3.3.1防治温度裂缝的措施:
3.3.1.1屋面设置保温层,减小温度变形;屋盖施工尽量做好保温层。
3.3.1.2屋面、挑檐可采取留置伸缩缝,或在屋面与砖墙间设置滑动面,以减少屋面伸缩对墙体的影响。
3.3.1.3对房屋较长、平面形状较复杂、构造和刚度不同的房屋,可每隔一定的距离将屋盖、楼盖、墙体或其他有关构件断开,形成若干较小的单元,每个单元因温度变形和收缩产生的拉力大大减小,从而防止裂缝的出现。
3.3.1.4提高砂浆强度,保证砌筑质量,在易开裂处设置水平拉接钢筋承受拉力。
3.3.2砌体的干缩变形引起的墙体开裂,可采取下列措施:
3.3.2.1在屋盖的适当部位设置控制缝,控制缝的间距不大于30m。
3.3.2.2当采用现浇混凝土挑檐的长度大于12m时,宜设置分格缝,分格缝的宽度不应小于20mm,缝内用弹性油膏嵌缝。
3.3.2.3建筑物温度伸缩缝的间距除应满足“设计规范”的规定外,宜在建筑物墙体的适当部位设置控制缝,控制缝的间距不宜大于30m。
3.3.3防止主要由墙体材料的干缩引起的裂缝可采取下列措施:
3.3.3.1在墙的高度、厚度不大于离相交墙或转角墙允许接缝距离之半、突然变化处及门、窗洞口的一侧或两侧设置竖向控制缝。
3.3.3.2竖向控制缝,对3层以下的房屋,应沿房屋墙体的全高设置;对大于3层的房屋,可仅在建筑物1-2层和顶层墙体的上述位置设置。
3.3.3.3控制缝在楼、屋盖处可不贯通,但在该部位宜作成假缝,以控制可预料的裂缝。
3.3.3.4控制缝作成隐蔽式,与墙体的灰缝相一致,控制缝的宽度不大于12mm,控制缝内应用弹性密封材料,如聚氨脂或硅树脂等填缝。
3.3.3.5控制缝的间距:对有规则洞口外墙不大于6mm;对无洞墙体不大于8m及墙高的3倍;在转角部位,控制缝至墙转角的距离不大于4.5m。
4.厨房及卫生间的地面渗漏的治理的治理的治理
4.1渗漏的原因分析
4.1.1管道周边预留洞口堵塞不当或不认真,砼未捣密实或未认真养护。
4.1.2预留洞位置不准,管道安装时扩孔造成孔周边砼松动并出现裂缝。预留孔洞的盒子在砼初凝后过早取出,用于下层的施工,使砼散裂,造成管根部渗漏。
4.1.3厨房、卫生间墙面和地面交接处出现空鼓、开裂导致渗漏。
4.1.4厨房、卫生间未按强制标准设置砼踢脚挡沿,容易造成墙面返潮和渗漏。
4.1.5烟囱、管道与地面交接处的处理不当同样会造成渗漏。
4.1.6墙面防水高度不足,造成墙面泅水。
4.1.7地面排水坡度小或地漏过高,使落水不能及时排走,出现积水现象。管道接口连接不紧密或排水不畅通,管道材料质量有问题,均会造成管件渗水跑漏。
4.2治理措施
4.2.1在卫生间、厨房四周墙体下部做高240mm的素砼挡沿,与现浇楼板一次浇捣,不留施工缝,为防水创造很有利的条件。
4.2.2施工前,要根据厨房、卫生间的卫生设备布局,对上给水、排水和通风等管道进行综合考虑,绘出详细施工坐标图,依据轴线精确定出预留洞位置,待砼终凝前再进行二次校核。这样就可以避免二次剔凿砼。
4.2.3预埋套管高度要大于50mm。
4.2.4预留洞封闭:管道固定好后,管道与预留洞的空隙用托模(或吊模)支模,清除疏松的砼并清理干凈并及时灌入砂浆、细石砼,避免长时间不施工灰尘杂物落入。将管子套管外壁满刷一度107胶水泥浆,并用10~20mm厚1:2水泥砂浆将洞边捣实,再将C20细石砼(内掺如有硅醇防水剂:水=1:12拌制)灌入模内,砼表面比洞口低20mm,用小铁棍轻轻捣实,24h内不准碰动,养护1~2天。
4.2.5拆模后,吊模的铁丝从跟部剪去,防止锈蚀后水沿铁丝渗漏,铁丝头用水泥砂浆抹平,待其硬化后,刷防水涂料一道,再用1:2水泥砂浆抹平。
4.2.6卫生间最好采用高分子防水卷材或者防水涂料,容易保证质量,泛水粘贴高度不低于300mm,有淋浴或洗涤存在浇淋的墙面,防水高度应超过其影响范围。
4.2.7防水层做好后,要进行不少于24h蓄水试验,发现问题。查清原因,及时处理。
4.2.8在管子根部粉出高于30mm以上的锥体。可以说,预留洞的处理是厨房、卫生间刚性防水的重点,在施工中引起高度重视。
4.2.9做好工序交接,铺地砖或贴瓷砖时不得破坏防水层,并保证排水坡度不少于1%,确保用户使用时不出问题。
5.质量通病的防治组织措施
以上仅列举几例质量通病,但质量通病对工程的影响可谓不小,经常发生的质量问题,有的是施工不认真,有的是材料不过关,有时是保护不当造成的,应从以下几方面做好工作:
5.1只有领导重视,全员参与,才能把质量问题消除在萌芽状态。
5.2合理安排施工顺序,作好成品保护。
5.3做好季节施工准备工作,做好夏季防雨排水和冬期的防冻工作。
5.4根据工程的具体特点,结合以往的经验教训,有所侧重的进行预防。
5.5设立质量通病攻关小组和奖励机制,狠抓落实。
5.6出现质量通病时,当原因较为复杂时,应组织技术人员进行会诊,查明原因,对症下药。
5.7质量通病的治理,要做到经济上合理,措施上可行并便于施工。
6.结语
随着住宅建筑工程的不断发展,一些经常发生的住宅工程质量问题,往往未能引起工程技术人员的重视而导致很多住户对住宅工程质量的不满意,涉及住宅质量通病的投诉越来越多,为提高住宅工程质量,必须对住宅质量通病进行全面深入的分析,并及时做好预防和治理,这样才能建设人们满意放心工程。
参考文献:
[1] 王剑英,牟建华.对外墙体外保温系统质量问题的分析[J]. 民营科技. 2010(04)
[2] 金鑫,李东岩.如何防治砌体工程施工中易发生的质量问题[J]. 黑龙江科技信息. 2010(13)
[3] 张康强.建筑施工中存在的常见问题及防治措施[J]. 科技资讯. 2006(08)
[4] 周建荣.浅谈现浇框架结构工程施工要点[J]. 科技资讯. 2007(15)
[5] 荆会忠.砌体裂缝的原因及防治措施[J]. 科技资讯. 2006(04)
关键词:质量通病;危害性;原因分析;治理技术;要点;重视
Abstract: In order to ensure that people of residential engineering quality requirements, we in the housing project construction process, strict requirements, in accordance with the standards of operation, and to strengthen the management, as far as possible, to strengthen the quality defects prevention and treatment, residential project quality common fault can be eliminated or avoided. This article mainly aims at the present building construction, residential projects in some of the common quality fault and prevention technology to conduct a comprehensive study.
Key words: quality; harm; cause analysis; control technology; key points; attention
中圖分类号:TU71献标识码: A 文章编号:2095-2104(2012)12-0020-02
1.住宅工程质量的危害性及防治对策
随着我国住宅基本政策和制度由公有化福利型向商品化市场型转变,使得与住宅的建设、质量、维修等有关法律维权的人也越来越多。老百姓用一辈子的积蓄买上一套商品住宅不容易,所以对居住环境和住宅质量的要求不断提高,为了提高住宅工程质量,满足住户对住宅工程质量不断完善的预期,住宅工程的质量是“百年大计”,与人民生命财产休戚相关。近年来,住宅工程质量通病导致的影响主体结构安全和影响使用功能已成为引起住户投诉的焦点,所以作为设计单位、建设单位、监理单位、施工单位各方的专业技术管理人员必须重视住宅工程质量,尤其是施工单位项目负责人和工程技术人员,掌握治理住宅质量通病的技巧,住宅工程质量一定会得到大大提升。
2.水泥地面起砂和空鼓的治理
2.1材料因素
2.1.1使用了水泥标号低或水泥受潮而降低了水泥强度等度的水泥。
2.1.2砂子含泥量大,颗粒过细,造成水灰比加大,强度降低。
2.2施工原因及防治
2.2.1使用强度不低于42.5级水泥,砂子采用中砂,细度模数为2.3~3.0。
2.2.2没有掌握压光时间和压光遍数;由于不掌握水泥硬化的机理,压光过早,水泥凝胶未形成,游离水过多,压光只是形成水光,其强度和抗磨能力不好;水泥终凝后再压光,操作困难并影响已硬化的表面,大大降低面层的强度和抗磨能力;水泥地面压光应在水泥终凝前,压光遍数一遍为2~3遍。
2.2.3水灰比大,砂浆强度降低容易造成起砂,控制好砂浆稠度。
2.2.4冬期施工砂浆受冻,强度降级容易造成起砂。
2.2.5养护不当,未到24h就浇水或地面缺水影响水泥的水化作用;养护时间不到就上人走动或进行下道工序的施工,造成地面的破坏和起砂。
2.2.6基层表面未清理干净,有浮灰和其它污物,影响与基层结合粘接,造成空鼓。
2.2.7垫层基层表面有积水也影响面层与基层的粘接力,造成空鼓。
2.2.8基层润湿不够,刷浆过早,造成风干硬结而形成隔离层。刷浆不均匀,存在干灰点也容易空鼓。
2.2.9砂浆层过薄,养护不及时,造成失水过快,影响与基层粘接造成空鼓,造成收缩干裂空鼓。
3.砌体裂缝和渗漏的治理
由于建筑物墙体裂缝、渗漏涉及的纠纷或官司越来越多,建筑物墙体裂缝已成为住户评判建筑物安全的一个非常直观、敏感和首要的质量标准。
3.1原因分析
引起砌体结构墙体裂缝的因素很多,既有地基、温度、干缩,也有设计上的疏忽、施工质量、材料不合格及缺乏施工经验等。
3.2砌体裂缝的种类
3.2.1八字型裂缝:
当外界温度上升时,外纵墙本身沿长度方向将有所伸长,但屋盖部分的伸长量比墙体的伸长量大得多,从而对墙体产生附加水平推力,墙体受到屋盖的推力而产生剪应力,剪应力和拉力又引起主拉应力。当主拉应力过大时,将在墙体上产生八字型裂缝,如在门窗洞边的八字型裂缝。
3.2.2水平裂缝和包角裂缝:
由于屋面伸长或缩短引起的向外或向内的推力产生的屋面板部或顶层圈梁下沿砖(砌块)灰缝的水平裂缝和砼平屋盖房屋顶层两端的墙体上包角裂缝。
3.2.3女儿墙裂缝:
由于屋面板和水泥砂浆面层发生过大温度变形,使女儿墙根部受到向外或向内的水平作用力而引起的女儿墙根部与平屋面交接处砌体外凸或女儿墙外倾所产生的裂缝。
3.2.4垂直裂缝:
当房屋的楼(屋)面为现浇钢筋混凝土结构时,由于收缩和降温引起的楼(屋)面缩短受到了墙体的限制,使楼(屋)面构件处于受拉状态。如果房屋过长,或设计时按采暖考虑而实际上未采暖,则可能在楼(屋)面上每隔一定距离发生贯通全宽的裂缝,在四个角发生八字型裂缝。当房屋有错层时,错层处的墙体容易产生局部的垂直裂缝。
3.2.5干缩裂缝:
烧结粘土砖,包括其它材料的烧结制品,其干缩变形很小,且变形完成比较快。只要不使用新出窑的砖,一般不要考虑砌体本身的干缩变形引起的附加应力。但对这类砌体在潮湿情况下会产生较大的湿胀,而且这种湿胀是不可逆的变形。对于砌块、灰砂砖、粉煤灰砖等砌体,随着含水量的降低,材料会产生较大的干缩变形,但是干缩后的材料受湿后仍会发生膨胀,脱水后材料会再次发生干缩变形,但其干缩率有所减小,约为第一次的80%左右。这类干缩变形引起的裂缝在建筑上分布广、数量多、裂缝的程度也比较严重。
3.3砌体裂缝的控制措施
3.3.1防治温度裂缝的措施:
3.3.1.1屋面设置保温层,减小温度变形;屋盖施工尽量做好保温层。
3.3.1.2屋面、挑檐可采取留置伸缩缝,或在屋面与砖墙间设置滑动面,以减少屋面伸缩对墙体的影响。
3.3.1.3对房屋较长、平面形状较复杂、构造和刚度不同的房屋,可每隔一定的距离将屋盖、楼盖、墙体或其他有关构件断开,形成若干较小的单元,每个单元因温度变形和收缩产生的拉力大大减小,从而防止裂缝的出现。
3.3.1.4提高砂浆强度,保证砌筑质量,在易开裂处设置水平拉接钢筋承受拉力。
3.3.2砌体的干缩变形引起的墙体开裂,可采取下列措施:
3.3.2.1在屋盖的适当部位设置控制缝,控制缝的间距不大于30m。
3.3.2.2当采用现浇混凝土挑檐的长度大于12m时,宜设置分格缝,分格缝的宽度不应小于20mm,缝内用弹性油膏嵌缝。
3.3.2.3建筑物温度伸缩缝的间距除应满足“设计规范”的规定外,宜在建筑物墙体的适当部位设置控制缝,控制缝的间距不宜大于30m。
3.3.3防止主要由墙体材料的干缩引起的裂缝可采取下列措施:
3.3.3.1在墙的高度、厚度不大于离相交墙或转角墙允许接缝距离之半、突然变化处及门、窗洞口的一侧或两侧设置竖向控制缝。
3.3.3.2竖向控制缝,对3层以下的房屋,应沿房屋墙体的全高设置;对大于3层的房屋,可仅在建筑物1-2层和顶层墙体的上述位置设置。
3.3.3.3控制缝在楼、屋盖处可不贯通,但在该部位宜作成假缝,以控制可预料的裂缝。
3.3.3.4控制缝作成隐蔽式,与墙体的灰缝相一致,控制缝的宽度不大于12mm,控制缝内应用弹性密封材料,如聚氨脂或硅树脂等填缝。
3.3.3.5控制缝的间距:对有规则洞口外墙不大于6mm;对无洞墙体不大于8m及墙高的3倍;在转角部位,控制缝至墙转角的距离不大于4.5m。
4.厨房及卫生间的地面渗漏的治理的治理的治理
4.1渗漏的原因分析
4.1.1管道周边预留洞口堵塞不当或不认真,砼未捣密实或未认真养护。
4.1.2预留洞位置不准,管道安装时扩孔造成孔周边砼松动并出现裂缝。预留孔洞的盒子在砼初凝后过早取出,用于下层的施工,使砼散裂,造成管根部渗漏。
4.1.3厨房、卫生间墙面和地面交接处出现空鼓、开裂导致渗漏。
4.1.4厨房、卫生间未按强制标准设置砼踢脚挡沿,容易造成墙面返潮和渗漏。
4.1.5烟囱、管道与地面交接处的处理不当同样会造成渗漏。
4.1.6墙面防水高度不足,造成墙面泅水。
4.1.7地面排水坡度小或地漏过高,使落水不能及时排走,出现积水现象。管道接口连接不紧密或排水不畅通,管道材料质量有问题,均会造成管件渗水跑漏。
4.2治理措施
4.2.1在卫生间、厨房四周墙体下部做高240mm的素砼挡沿,与现浇楼板一次浇捣,不留施工缝,为防水创造很有利的条件。
4.2.2施工前,要根据厨房、卫生间的卫生设备布局,对上给水、排水和通风等管道进行综合考虑,绘出详细施工坐标图,依据轴线精确定出预留洞位置,待砼终凝前再进行二次校核。这样就可以避免二次剔凿砼。
4.2.3预埋套管高度要大于50mm。
4.2.4预留洞封闭:管道固定好后,管道与预留洞的空隙用托模(或吊模)支模,清除疏松的砼并清理干凈并及时灌入砂浆、细石砼,避免长时间不施工灰尘杂物落入。将管子套管外壁满刷一度107胶水泥浆,并用10~20mm厚1:2水泥砂浆将洞边捣实,再将C20细石砼(内掺如有硅醇防水剂:水=1:12拌制)灌入模内,砼表面比洞口低20mm,用小铁棍轻轻捣实,24h内不准碰动,养护1~2天。
4.2.5拆模后,吊模的铁丝从跟部剪去,防止锈蚀后水沿铁丝渗漏,铁丝头用水泥砂浆抹平,待其硬化后,刷防水涂料一道,再用1:2水泥砂浆抹平。
4.2.6卫生间最好采用高分子防水卷材或者防水涂料,容易保证质量,泛水粘贴高度不低于300mm,有淋浴或洗涤存在浇淋的墙面,防水高度应超过其影响范围。
4.2.7防水层做好后,要进行不少于24h蓄水试验,发现问题。查清原因,及时处理。
4.2.8在管子根部粉出高于30mm以上的锥体。可以说,预留洞的处理是厨房、卫生间刚性防水的重点,在施工中引起高度重视。
4.2.9做好工序交接,铺地砖或贴瓷砖时不得破坏防水层,并保证排水坡度不少于1%,确保用户使用时不出问题。
5.质量通病的防治组织措施
以上仅列举几例质量通病,但质量通病对工程的影响可谓不小,经常发生的质量问题,有的是施工不认真,有的是材料不过关,有时是保护不当造成的,应从以下几方面做好工作:
5.1只有领导重视,全员参与,才能把质量问题消除在萌芽状态。
5.2合理安排施工顺序,作好成品保护。
5.3做好季节施工准备工作,做好夏季防雨排水和冬期的防冻工作。
5.4根据工程的具体特点,结合以往的经验教训,有所侧重的进行预防。
5.5设立质量通病攻关小组和奖励机制,狠抓落实。
5.6出现质量通病时,当原因较为复杂时,应组织技术人员进行会诊,查明原因,对症下药。
5.7质量通病的治理,要做到经济上合理,措施上可行并便于施工。
6.结语
随着住宅建筑工程的不断发展,一些经常发生的住宅工程质量问题,往往未能引起工程技术人员的重视而导致很多住户对住宅工程质量的不满意,涉及住宅质量通病的投诉越来越多,为提高住宅工程质量,必须对住宅质量通病进行全面深入的分析,并及时做好预防和治理,这样才能建设人们满意放心工程。
参考文献:
[1] 王剑英,牟建华.对外墙体外保温系统质量问题的分析[J]. 民营科技. 2010(04)
[2] 金鑫,李东岩.如何防治砌体工程施工中易发生的质量问题[J]. 黑龙江科技信息. 2010(13)
[3] 张康强.建筑施工中存在的常见问题及防治措施[J]. 科技资讯. 2006(08)
[4] 周建荣.浅谈现浇框架结构工程施工要点[J]. 科技资讯. 2007(15)
[5] 荆会忠.砌体裂缝的原因及防治措施[J]. 科技资讯. 2006(04)