论文部分内容阅读
cBN,α-Si3N4,AlN and Al2O3 sintered with Y2O3 as additives under 5.5GPa at 1500℃~1700℃ for 20min.The samples were observed by X-ray diffraction,scanning electron microscopy,TEM and HRTEM.