1986年4月,绍兴瓷厂新建的面砖辊道窑投产。当时采用了适宜于多孔窑烧成的喷釉工艺。由于釉层薄,颗粒粗,烧成后的产品波纹多,背面易粘釉,严重影响产品的外观质量。经向有关科研单位讨教、求援,得到的答复是。面砖背面粘釉是个通病,目前在国外也是个难题。在厂领导和工人的有力支持下,与瓷土打交道达30年之久的金福仁老师傅下决心解决这个难题。经三个月的探索试验,终于找到了办法——在龙骨带上加钉子,使面砖与龙骨带隔离,使其减少接触,不但顺利地解决了粘
In April 1986, the new brick roller kiln built by Shaoxing Porcelain Factory went into operation. At that time, a glaze spraying process suitable for firing the porous kiln was used. Because the glaze layer is thin and the particles are coarse, the product ripples after firing, and the back surface is easily glazed, which seriously affects the appearance quality of the product. After consulting the relevant scientific research units for assistance, the answer is: The glazed glaze on the back of the tile is a common problem, and it is also a problem in foreign countries. With the strong support of factory leaders and workers, Master Jin Furen, who has been dealing with China for 30 years, is determined to solve this problem. After three months of exploration and experimentation, we finally found a way to add nails to the keel belt to isolate the face bricks from the keel belt so as to reduce contact and not only successfully resolve the stickiness.