Nanofibers of alpha silicon nitride were grown by a vapor-solid mechanism at 1450?C, through the carbothermal reduction process. Two different precursor silica
Zirconia oxide (ZrO2) nanofibers were synthesized using Phosphorus/water mixture as catalyst by ultrasonic spray pyrolysis CVD on the zirconia substrate at 900&