废旧模具的再生

来源 :机械工人 | 被引量 : 0次 | 上传用户:wisdom76
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
液化石油气钢瓶封头的落料模(尺寸见图)在使用中,由于刃口磨损,使凸模尺寸变小,凹模尺寸变大。当凸、凹模的间隙超过0.8mm时,就得更换新模具,我厂自生产钢瓶以来,已报废4个凹模、1个凸模。为节约材料和资金,我们将已报废的模具进行改制,从而节省了资金2万多元,具体做法如下:将4个四模内腔进行磨削,尺寸扩大到φ645_0~(+0.07)mm,并配制一个新凸模,尺寸为φ644.7_(-0.07)~0mm。又将废凸模尺寸磨削到φ643.7_(-0.07)~0mm,并配制两个新凹模,尺寸为 Liquefied petroleum gas cylinder head blanking die (size see picture) in use, due to the wear of the blade, the punch size becomes smaller, the die size becomes larger. When the convex and concave die gap exceeds 0.8mm, you have to replace the new mold, I plant since the production of cylinders, has been scrapped four die, a punch. In order to save materials and capital, we will have scrapped the mold for restructuring, thus saving more than 20,000 yuan of funds, as follows: The four four-cavity mold grinding, the size expanded to φ645_0 ~ (+0.07) mm, And the preparation of a new punch, the size of φ644.7 _ (- 0.07) ~ 0mm. Again the size of the punch punch grinding to φ643.7 _ (- 0.07) ~ 0mm, and the preparation of two new die, the size of
其他文献
一战姚家峪2006年夏天,听钓友说,云蒙湖姚家峪出鲤鱼,每天少则几千克,多则能钓二三十千克鱼。听到这个消息,我兴奋不已,经过几天的准备之后, World War I Yaojiayu summer 2
轻工部门制造揿钮、鞋眼及电珠头等日用小商品都采用黄铜皮加工后电镀,这样做成本高,工序复杂,需要消耗大量的钢材。因此出现了目前压延和拉伸用的ZnCu1.5合金。 ZnCu1.5合
电火花加工中钢打钢时电极损耗时大、时小。怎样在加工中及时控制电极损耗,使之减小到最小程度,是人们共同探讨和研究的课题,我们谈一些经验及看法。我们在晶体管脉冲电源,
我厂750型旅游面包车左、右半轴上的花键原在铣床上加工,因分度误差较大,改在631K花键铣上加工。但631K的最大加工长度为600mm,工件长度为706 mm。为此,我们取下床头箱上的内
制作柴油机气门用的模具,属于热作模。气门是局部加热后在摩擦压力机上热镦成型的,因此要求模具具有较好的热疲劳性和热强性,一般多采用3Cr2W8V钢来制造。根据型号不同,模具
对大模数淬火齿轮,各厂家多采用中频感应淬火。我厂引进西德派纳公司的液压技术,生产多种电动液压抓具,其齿端驱动臂(图1)采用单齿双面高频淬火。感应器用10×6mm矩形紫铜管
可移带式松砂机松砂皮带跑偏的问题是普遍存在的,它不仅影响使用效果,而且增加了皮带和皮带轮的磨损,严重地影响了使用寿命。如何解决松砂皮带的跑偏问题?松砂皮带跑偏,是由
众所周知,一般插齿机加工的齿轮,普遍存在周节偏差较大的问题。特别是贯彻国家新标准 GB 4686-84插齿机精度标准以来,插削齿轮的周节偏差要求达到JB 179-83齿轮新标准6级精度
长期以来,绝大部分工厂铸造生产的混砂工艺为:先加入原砂和膨润上等进了了干混,然后再加水或水玻璃等进行湿混,以便尽快达到所要求的型砂性能。可是,实际上这样的加料顺序,不
教师被人们比喻成燃烧自己照亮别人的蜡烛,哺育人们心灵的工程师,先贤圣哲等。她是传授知识、启迪心灵、传播文明的使者,每一个人的学习、生活、成长以及成功都离不开老师的