【摘 要】
:
上钢五厂铸锭采用绝热帽口提高了钢锭质量,减少了缩孔废品,成坯率有所提高。但因绝热板成本高,以及粉状脱落污染环境等问题而影响推广应用。23号配方绝热帽改型研制成功,效
论文部分内容阅读
上钢五厂铸锭采用绝热帽口提高了钢锭质量,减少了缩孔废品,成坯率有所提高。但因绝热板成本高,以及粉状脱落污染环境等问题而影响推广应用。23号配方绝热帽改型研制成功,效果十分显著,有利于纤维绝热帽推广应用。 23~#配方绝热帽的特点: 1.保温效率和纤维绝热板相近,略差于
On the steel plant five ingot adiabatic hatch ingot to improve the quality of ingot to reduce the shrinkage of shrinkage, into the billet rate has increased. However, due to the high cost of insulation panels, as well as the pollution of powder off the environment and other issues affect the promotion and application. No.23 formula insulation cap modified successfully developed, the effect is very significant, is conducive to the promotion of fiber insulation cap. 23 ~ # formula insulation cap features: 1. Insulation efficiency and fiber insulation panels are similar, slightly worse than
其他文献
上钢三厂电炉车间推行喷粉快白渣还原新工艺取得显著效果。该车间自1981年11月至1982年1月共进行九十七炉四个钢种的新工艺试验,经总结经验并适当调整工艺后,从1982年3月起,
中国金属学会第三届第五次常务理事会议于1983年1月5~6日在北京召开.有36位常务理事出席.陆达、李董、张文奇、黄培云副理事长分别主持了会议.这次常务理事会议的主要内容是:
由中国金属学会和国家科委钢铁冶金组联合召开的我国钢铁工业技术改造专家讨论会,于1982年12月23~29日在武汉钢铁公司举行.出席这次会议的有科研、设计单位,高等院校,厂矿企
八二年十一月中旬,冶金职大开办“质量管理干部业务进修班”,为期二个半月。参加该“业务进修班”的有冶金局所属各厂的质量管理干部和浙江、江苏冶金系统有关同志。“进修
国际选矿和提取冶金学术会议,已由英国采矿冶金学会发出第一次通知,主要内容是:这次国际会议由采矿冶金学会和中国金属学会筹备,于1984年10月14日至20日在中华人民共和国云
云锡公司第三冶炼厂对锡中矿采用高温氯化挥发所得湿式收尘溶液,是一种含砷高也含有多种有价金属离子且浓度极低的氯化物溶液,其成份为(克/升):Cu0.80、Zn19.46、Bi1.02、Cd
1982年6月,索尔梅公司福斯厂2号高炉全焦操作,无辅助燃料,每吨生铁只需439公斤焦炭,创炼铁热消耗的世界新纪录。索尔梅公司的2号高炉,炉缸直径2米,总容积为2850米~3。经五个
机械工业部通用基础件工业局粉末冶金行业第四次产品质量评比及大区行业组长会议于1984年5月28日至6月1日在山西省大同市召开。共29个单位45名代表参加了会议。会议按照有关
中国金属学会轧钢学术委员会工作会议于1984年6月16~17日在北京召开。中国金属学会副秘书长康文德同志及轧钢学术委员、各学术组有关人员等共26人参加了会议。会议首先对去年
(一)标准化是一项综合性的基础工作,对促进技术进步,实现我国社会主义现代化建设的宏伟目标具有重要作用。目前的国际标准和国外先进标准反映了经济发达国家七十年代或八十