论文部分内容阅读
К.С.Ассанович等曾用分选机样机进行了各种有用矿物的光电分选试验,证明,在工业中采用该设备组成的工艺过程是有前途的。用三种试料即:破碎后经重介质选别所得的轻产品(试料1)、开路循环自磨的矿石(试料2)和闭路自磨的矿石(试料3)。送入光电分选机选别的全部试料入选粒度为-50和+18毫米,试验结果见表。
К.С.Ассанович and other prototype machines have been used for a variety of useful mineral photoelectric classification test to prove that in the industrial use of the equipment consisting of the process is promising. Three samples were obtained: light product (sample 1) obtained after crushing by medium selection, sample (sample 2) with open-cycle self-grinding, and ore with closed-circuit self-grinding (sample 3). Selected into the optical sorting machine selected all the selected particles size of -50 and +18 mm, the test results shown in the table.