To build the relationship between solidification conditions and the interfacial bond strength,Al2O3f/Al-15Si composite solidified at different cooling rates wer
Ni83Fe17 films with a thickness of about 100 nm were deposited on thermal oxidized silicon substrates at ambient temperature, 240, 350, and 410℃ by DC magnetro
RuS2 thin films were prepared by the cost-effective chemical method-successive ionic layer adsorption and reaction (SILAR). The structural, optical, and electri
The inhibition effects of sodium vanadate along with inorganic coolant inhibitors were examined on corrosion of AZ91D in ASTM D1384-80 corrosive water by polari
The influence of pre-annealing on thermal stability of the amorphous Zr70Cu20Ni10 alloy was reported by employing the differential scanning calorimetry (DSC) an