论文部分内容阅读
梅山集团公司1995年的重点科研攻关项目——梅山铁精矿选磷工业试验,经试验小组近一年的努力,于1995年12月全部结束。试验是按“浮—磁—浮”和“浮—磁—强磁”两个流程进行的。“浮—磁—浮”流程最终铁精矿:T_(Fe)54.71%,S0.37%,P0.243%,铁金属作业回收率96.45%;“浮—磁—强磁”流程最终铁精矿:T_(Fe)56.08%,S0.29%,P0.246%,铁的作业回收率94.65%。两个试验结果均达到了公司“承包协议”所要求的技术指标。
Meishan Group Corporation in 1995 key scientific research project - Meishan iron concentrate phosphorus industrial test, the test group nearly a year of efforts, in December 1995 all over. The test is based on “float - magnetic float ” and “float - magnetic - Ferromagnetic ” two processes. “Float - magnetic - float ” process final iron concentrate: T_ (Fe) 54.71%, S0.37%, P0.243%, iron metal recovery rate 96.45% The final iron concentrate process: T_ (Fe) 56.08%, S0.29%, P0.246%, iron recovery rate of 94.65%. The two test results have reached the company “contract agreement ” the required technical indicators.