Appliction of MgO0-Cr2O3 brick composed of MgO>72%,Cr2O3>14.8%-168.69%,with porosity 13%-14%,compressive strength 33.0-43.8 MPa, flexure strength 11.9-16.5 MPa and refractoriness under load ≥1750℃ in an assemble snorkel of 300t RH furnace in Baoskh