论文部分内容阅读
用硅铝热法在小容量镁坩埚炉里进行冶炼试验,获得了比重小、熔点低、含钨35%,含钼30%左右的钨钼复合铁合金,为工业性试验摸索了方法和条件。
The smelting experiments were carried out in a small capacity magnesium crucible furnace by the aluminosilicate thermal method, and the tungsten-molybdenum composite ferroalloy with small specific gravity, low melting point, 35% tungsten and about 30% molybdenum was obtained. The methods and conditions were explored for industrial experiments.