The hot deformation characteristics of TiC particles reinforced titanium matrix composite were studied in the temperature range from 900 ℃ to 1 150 ℃ and in t
The VCp reinforced stainless steel composite was produced by in-situ reaction casting. The composite was tested for its wear resistance under the wet abrasive c
Ni80 Fe20 films with thickness about 54 nm were deposited on K9 glass and thermally oxidized silicon substrates at ambient temperature by electron beam evaporat
<正>The effects of Sr element on the forming properties of the Al-Mg-Si based alloy sheets were studied by tensile test, metallograph, DSC, XRD, SEM and TEM. Th