甘肃主要火电厂,拥有钢球磨煤机四十多台,年耗钢球,钢衬瓦,锤头三千余吨,以钢球消耗最多,磨一吨煤粉平均耗球500~800克。有的电厂高达1194克。为了探讨其磨损问题,于一九七七年开始试验研究。一、综合选材: 经过试验研究,证明采用45Mn_2钢是制造耐磨件的材料,与过去使用的高碳,高合金的钢种相比,由于45Mn_2钢属中碳低合金冶炼较易,锰在钢中有一定的固溶度,形成锰铁 The main thermal power plant in Gansu, with more than 40 ball mill coal mills, annual consumption of steel balls, steel lining tile, more than 3,000 tons of hammer to steel balls consume the most, grinding a ton of coal powder consumes an average of 500 to 800 grams. Some power plants up to 1194 grams. In order to explore its wear and tear problems, a pilot study was started in 1977. First, the comprehensive selection: After the pilot study showed that the use of 45Mn2 steel wear-resistant parts of the material, compared with the past use of high-carbon, high alloy steel, 45Mn2 steel due to low-carbon smelting easier, manganese in Steel has a certain degree of solid solubility, the formation of ferromanganese
其他文献
医学英语是科技英语的一个分支,具有科技英语的一些特点:专业词汇多,长句、套句出现频率高;多用被动语态、名词化和分词短语;多用并列结构等。因此,要想把医学英语文章译成既忠实于
金属螯合物形成反应的研究受到很大的重视。而氨羧络合剂对相同电荷但半径不一的相似离子的特殊选择性已成为用离子交换法分离该类离子的基础。 最近,我们报道了属于EDTA类
前言环氧粉末涂料是六十年代发展起来的一种新材料。它主要是由环氧树脂、固化剂、颜料、填料及添加剂组成的热固性粉末涂料。在热固性粉末涂料中,它发展得最早,产量一直居
在大型球铁铸件浇注时,如果注意以下几点,就可以使非金属夹杂减少到最低限度。这是根据123个铸铁轧辊的实验得出的结论。这些措施是: 1.在铁水中加入0.05%的冰晶石。 2.浇注
由于使用领域的扩大,对镀锌材料的塑性、耐蚀性和可焊性提出了高要求,同时还要求增强漆层的附着力。用来涂漆的锌层,例如生产成型盖板,锌层的厚度就可以薄一些。带有复合涂
一、对标准的说明西德模锻件公差标准DIN7526和英国的标准BS4114是一致的,都是在“欧洲锻造”技术委员会建议制订而以本国标准的型式颁布的。“标准”只控制钢锻件的尺寸精
一、前言我们曾用粉末压片的方法测定镍矿尾矿中的镍和铜,对铜取得了满意的结果。但由于镍矿难于磨细,颗粒度效应和均匀性影响使镍的分析结果不够理想。本文采用溶液法,消除
一、前言由于电磁振动给料机具有结构简单,操作维护方便,功率消耗少,给料均匀,便于实现给料量的自动控制等优点,在轻重工业各部门都得到了广泛的应用。我国于1970年4月,在河
铝箔轧制用的工艺润滑油,一般是由基础油和添加剂所组成。前者主要起载体和冷却作用,后者起润滑作用以获得压下量,在现代高速轧制技术的发展中,由于速度效应使铝箔轧制可获
本文提出一种新的X射线形貌法,并利用它观察三点弯曲Mo单晶的断口特征及其断裂过程。从断口X射线衍射像中不但看到同金相断口一样的分区,即失稳扩展区、稳态扩展区和由撕裂形