论文部分内容阅读
To improve the initial corrosion resistance and then make the degradation rate of magnesium alloys to meet the biomedical application,two kinds of crack-free calcium phosphate glass-ceramic coating,namely CaOP2O5-SrO-Na2O and CaO-P2O5-Na2O-ZnO,were synthesized on AZ31B magnesium alloy substrates by sol-gel method using dip-coating technique,following the heat treatment in the temperature of 400-500℃.Ca2P2O7 first crystallized from the glass matrix as main phase during the heat treatment process.