黑硅的形貌对晶体硅电池性能影响研究

来源 :2018 年第十四届中国太阳级硅及光伏发电研讨会 | 被引量 : 0次 | 上传用户:wahyle
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
本文阐述了黑硅的形貌对晶体硅电池性能影响,黑硅虽然都可以达到陷光的目的,但不同的结构陷光机理不同;黑硅的后处理工艺,对于黑硅效率有着显著影响,不同的黑硅结构会对电池性能造成显著影响。
其他文献
Topological material has been intensively studied due to its novel properties.Meanwhile,the discovery and verification are always subject to density function theory(DFT)in theory and angle-resolved ph
会议
The increased interest in quantum phase transitions and the study of new magnetic state-skyrmions under pressure demands the creation of new non-magnetic high-pressure cells.High pressure clamp cells
会议
Far-infrared spectra can provide information about lattice dynamics of crystals,from which thermodynamic properties of the crystals can be derived.
会议
Under sufficiently high pressure one anticipates that the 4f state of a given lanthanide becomes unstable,leading to highly correlated electron effects and exotic physics.Recent four-point electrical
会议
A periodic arrangement of localized electron which hybiidize with conduction electrons,can lead to novel phenomena such as quantum criticality[1][2] and superconductivity[3].In particular,in heavy fer
会议
铸造单晶量产效率与直拉单晶差0.3%以内,157.75mm与单晶实现同瓦输出,价格低0.3-0.4元,给客户更高的性价比。氧含量最低到2ppma,低电阻率分布更加均匀,效率进一步提升0.2%。铸造单晶通过籽晶回用,大尺寸硅锭,薄硅片等方法,成本进一步下降。
本文阐述了光伏电站质量控制,确定环境条件、太阳资源、电气、土建及其它站址属性,从而确认满足初步设计目标,characteristics建立可参考的性能比,主要的项目为:光伏系统性能比(PR);DC系统运行评价。
本文阐述了钙钛矿薄膜组件的封装与挑战,通过降低层压温度,增加阻水率10-5g/m2/d,减少热膨胀幅度来提高封装效果。
本文阐述了高效晶硅光伏组件低封装损技术,搭配0.27mm焊带+白色EVA+3mm间距组合后组件功率没有单个材料单独使用带来的增益之和高,且单独使用白色EVA比单独使用加0.27mm焊带功率增益要高。搭配0.27mm焊带+0.45mm透明EVA的组件平均功率较0.5mmEVA提升0.4W左右,但碎片及隐裂不良率较高。
本文阐述了国产PVDF薄膜产业化现状和发展趋势,PVDF薄膜特性决定了它的耐候特性和25年寿命保障;中国有完整的氟化工产业链,足以支撑中国乃至全球光伏发展保护需要;国产PVDF薄膜的制造水平优于国外氟膜制造水平。