全苏金属制品科学研究院为了制定用不锈钢和电阻合金生产0.2-0.3毫米细丝的高效率方法,进行了一系列研究工作。这种方法可以确保在热处理和湿拉联合作业时金属丝获得流水线加工,从而免除了拉丝前金属丝的表面准备工序。采用快速电加热法(1000-4000℃/秒)以创造有利于再结晶过程进行的条件和线坯在流动的冷水由进行冷却的方法,可以使金属获得必需的工艺性能。在此条件下,金属具有所
All-Su Metal Products Research Institute conducted a series of studies to develop an efficient method for producing 0.2-0.3 mm filaments using stainless steel and a resistive alloy. This method ensures that the wire is pipelined during heat treatment and wet-pull joint operations, eliminating the need for surface preparation of the wire before drawing. Rapid electrical heating (1000-4000 ° C / s) is used to create the process conditions conducive to the recrystallization process and cooling of the strand in cold flowing water to achieve the necessary process performance of the metal. In this condition, the metal has