论文部分内容阅读
矿浆在150—230℃,在氧气存在下压煮,然后使氢氧化钠加入反应区,辉钼矿就转化成三氧化钼,转化反应继续进行直到 pH 从0.05升到0.5。然后再将含有三氧化钼为主的固体从泥浆中分离出
The slurry is boiled at 150-230 ° C in the presence of oxygen and then sodium hydroxide is added to the reaction zone where the molybdenite is converted to molybdenum trioxide and the conversion is continued until the pH is increased from 0.05 to 0.5. The solid containing molybdenum trioxide is then separated from the slurry