矿石为方鉛矿和閃鋅矿,在矿床的南部为白鉛矿和异极矿。生产能力为1000吨/昼夜的1号选矿厂有一个系統,而生产能力为4500吨/昼夜的2号选矿厂由三个相同系統(在浮选异极矿以前)組成,每一系統的生产能力为50吨/小时,两个系統选别硫化矿,一个系統选別氧化矿。还有一个生产能力为4吨/小时的半工业性选矿厂。交替地破碎硫化矿和氧化矿。在1号选矿厂处理含2%Pb和13—16%Zn的原矿,获得含69—70%鉛和61—62%Zn的精矿,共回收率分别为89—90%和96—97%。
The ores are galena and sphalerite, and in the southern part of the deposit are lead and hemimorphite. There is a system for the No. 1 concentrator, with a production capacity of 1000 tons / day and night, and the No. 2 concentrator, with a production capacity of 4,500 tons / day and night, consists of three identical systems (before the flotation of the hemimorphic mine), each producing Capacity of 50 tons / hour, two systems sorting sulphide ore, a system of sorting ore. There is also a semi-industrial concentrator with a production capacity of 4 tons / hour. Sulfur ore and oxide ore are broken alternately. In the No. 1 beneficiation plant, the ore containing 2% Pb and 13-16% Zn was processed to obtain concentrates containing 69-70% lead and 61-62% Zn. The total recoveries were 89-90% and 96-97% .