1997年,柳钢炼铁生产进步显著,生铁产量突破百万吨大关,达到100.8万t,比1996年净增22.2万t。技术经济指标明显改善,高炉利用系数达2.36t/m~3。d,比1996年提高0.54t/m~3.d;入炉焦比518kg/t,比1996年下降103kg/t。 1997年,柳钢炼铁取得上述明显进步采取的主要措施为: 1.进一步落实精料措施 1997年,柳钢进口了部分澳矿、南非矿、越南矿等,使入炉矿石品位提高。1996年,烧结厂2号烧结机投产,同时烧结厂开展各项
In 1997, Liuzhou Steel made significant progress in its iron and steel production. The output of pig iron exceeded one million tons, reaching 1.08 million tons, a net increase of 222,000 tons over 1996. Technical and economic indicators improved significantly, blast furnace utilization factor of 2.36t / m ~ 3. d, 0.54t / m ~ 3.d higher than that of 1996; the coke ratio into the furnace is 518kg / t, 103kg / t lower than that in 1996. In 1997, the major measures taken by Liuzhou Iron and Steel to make the above significant progress were as follows: 1. Further Implementation of Concentrate Measures In 1997, Liuzhou Iron and Steel imported some ore, South African mine and Vietnam mine to raise the quality of the ore that was put into the furnace. In 1996, sintering plant No. 2 sintering machine put into operation, while sintering plant to carry out