焙烧温度对甲醇氧化制甲醛铁钼催化剂结构及性能的影响

来源 :天然气化工:C1化学与化工 | 被引量 : 0次 | 上传用户:wqra555551q
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
以Fe(NO3)3·9H2O和(NH4)6Mo7O24·4H2O为Fe源和Mo源,通过共沉淀法制备了系列不同焙烧温度的铁钼催化剂,并考察了催化剂对甲醇氧化制甲醛反应性能的影响。结果表明,400℃焙烧的铁钼催化剂具有最佳催化性能,其甲醇转化率为96.6%、甲醛收率为87.6%、甲醛选择性为80.7%。进一步通过BET、XRD、Raman、SEM、XPS及H
其他文献
In the light of superior interaction between pyridine unit and perovskite,a facile star-shaped triphenylamine-based hole transport material(HTM)incorporating py
Lithium-sulfur (Li-S) batteries have become a promising candidate for advanced energy storage system owing to low cost and high theoretical specific energy.In t
Graphite as a promising anode candidate of K-ion batteries (KIBs) has been increasingly studied currently,but corresponding rate performance and cycling stabili
It is of vital importance to accelerate the sluggish oxygen reduction reaction (ORR) process at the cathode with earth-abundant metal-based catalysts for the co
A new catalyst of Co/La4Ga2O9 for CO2 hydrogenation to produce ethanol was prepared by reducing LaCo0.5Ga0.5O3,which showed excellent selectivity to ethanol (≈
Developing an efficient artificial photosynthetic system for transforming carbon dioxide and storing solar energy in the form of chemical bonds is one of the gr
Photovoltaic technology is a promising choice for human beings to solve critical environmental and energy problems. Much effort has been expended around the world on this technology which has allowed it to flourish, both in power conversion efficiency (PC
Designing low-cost,easy-fabricated,highly stable and active electrocatalysts for oxygen evolution reaction (OER) is crucial for electrochemical (EC) and solar-d
Surface-functionalized nitrogen/carbon co-doped polymorphic TiO2 phase junction nanoparticles uniformly distributed in porous carbon matrix were synthesized by
采用共沉淀法打片成型制备出铜锌铝系加氢催化剂,考察了反应条件对该催化剂催化醋酸乙酯加氢制乙醇活性和选择性的影响。结果表明,在反应温度220℃、压力2.5 MPa、氢酯物质的量比30、液空速1.0 h-1时催化剂性能最佳,醋酸乙酯转化率为96.2%,乙醇选择性为99.4%。结合BET、XRD、XPS等手段对反应前后的催化剂样品进行了表征,发现催化剂具有明显的介孔结构,最可几孔径约16 nm,比表面积为50~60 m2/g,Cu0为催化剂主要活