Heat treatment changes the structure of the cobalt binder phase and the properties of the WC-Co hardmetals. The higher the cobalt content in the alloy is, the m
Si3N4 ceramics with AZ-type non-toxic, non-oxide additives canbe highly densified. In this work densification behavior and mechanism ofSi3N4 with AZ-type additi