论文部分内容阅读
本文探讨锌-镍合金的合理镀液配方和电沉积工艺条件。用硫酸盐为镀液,以葡萄糖酸钠做络合剂,在添加剂Ⅰ与添加剂Ⅱ的作用下,获得了含镍15-20%的合金镀层。
This article discusses the reasonable zinc-nickel alloy plating bath formulation and electrodeposition process conditions. Using sulphate as plating solution and sodium gluconate as complexing agent, 15-20% nickel alloy coating was obtained under the action of additive Ⅰ and additive Ⅱ.