论文部分内容阅读
The alloy was reheated to 580℃ for tempering at rates of 2 , 5 , 10 , 20 , and 40℃ / s , respectively , after quenching.The amount , distribution , and stability of reversed austenite were investigated by X-ray diffraction ( XRD ) and electron back scatte