论文部分内容阅读
低热硅酸盐水泥(以下简称“低热水泥”)是以贝利特等低钙矿物为主要组分的水泥。与阿利特相比,贝利特形成温度低(1350℃即可大量形成)、热耗低(理论热耗1268k J/kg)。低钙硅酸盐水泥在生产过程中,石灰石消耗量小,熟料烧成温度降低50℃~100℃,CO2排放也大幅减少。随着人们对节约能源和降低温室气体排放越来越重视,特别是碳排放和碳交易逐渐走向市场,低
Low heat Portland cement (hereinafter referred to as “Low Heat Cement”) is a cement composed mainly of low-calcium minerals such as Belite. Compared with Alite, Bellete formation temperature is low (1350 ℃ can be formed in large quantities), heat consumption is low (theoretical heat consumption 1268k J / kg). Low calcium silicate cement in the production process, the consumption of limestone small, clinker firing temperature decreased by 50 ℃ ~ 100 ℃, CO2 emissions also dropped significantly. As people pay more and more attention to saving energy and reducing greenhouse gas emissions, especially as carbon emissions and carbon trading gradually move to the market, low