The solidified microstructure of immiscible alloys strongly depends on the nucleation, diffusional growth, especially the coalescence of the second phase drople
Si3N4 ceramic was jointed to Si3N4 ceramic using a filler alloy of Cu-Zn-Ti at 1 123-1 323 K for 0.3 -2.7 ks. Ti content in the Cu-Zn-Ti filler alloy was 15% (m