论文部分内容阅读
制备大输液加入活性炭时,常易造成粉末飞扬,污染用具及环境。为克服这一弊端,我们对加炭方法作了如下改进。取250ml盐水瓶洗净、干燥,称取适量活性炭装入瓶内(活性炭可根据原料重量及纯度酌定,一般用0.1~0.5%,以每瓶装量可处理一批次葡萄糖原料为宜)。将瓶置烤箱内120℃干燥2h,稍冷加塞密闭保存 (为避免每次称取的麻烦,可一次称取多瓶备用)。另取盐水瓶胶塞打孔,插入输血玻管一根,玻管上端套
Preparation of transfusion when adding activated carbon, often easily lead to powder flying, pollution and appliances and the environment. To overcome this shortcoming, we made the following improvements on the carbonation method. Take 250ml saline bottle washed, dried, weighed amount of activated carbon into the bottle (activated carbon according to the weight and purity of raw materials discretion, generally with 0.1 to 0.5%, in order to install a bottle per batch of glucose material suitable). The bottle was placed in the oven at 120 ℃ for 2h, slightly cold and stuffed tightly closed (in order to avoid the trouble of weighing each time, we can weigh more than one bottle at a time). Another saline bottle stopper hole, insert a transfusion glass tube, glass tube on the end of the sleeve