湘乡氟化盐厂中和槽循环送料φ4″砂泵,过去用石灰乳中和时一直采用油浸石棉盘根,在改用粘土矿矿浆中和游离硫酸后,由于介质温度高、泥浆比重大,石棉油浸盘根已不适应,压盘根成了中和槽工的主要负担,由于盘根压不住,大量高温含酸泥浆外溅,既不安全又恶化了劳动条件,并且影响生产工艺的流水作业。该厂经反复研究,改用“挡浆水环橡胶密封”,效果很好。其作法是:在 Xiangxiang fluoride salt in the tank and the tank circulating feed φ4 “sand pump, lime milk used in the past has been the use of oil asbestos packing, the switch to clay ore and free sulfuric acid, the medium temperature is high, the mud weight Large, asbestos oil pan packing has not adapted to the pressure into the root and the trough of the main burden, because the packing can not hold, a large number of high temperature acid mud splashing, neither safe and aggravated the working conditions, and the impact Production process of water operations. The plant after repeated studies, switch to ”block water ring rubber seal", the effect is good. The practice is: at
其他文献
我厂81台21号浮选机中的48台原设计使用有拔销的1213双列调心球轴承。这种轴承与竖轴固定是通过一个带有拔销的紧定套来实现的。多年来,由于这种紧定套的加工精度要求较高,
应用活性炭从银电解液中回收铂钯工业试验贵金属研究所与云南冶炼厂合作于一九七三年在实验室和工业性探索试验的基础上,一九七四年又针对应用于工业生产需要解决的问题,进
为了检查去年召开的技术革新会议精神贯彻情况,局革委会,于今年八月至十一月分别组织了对局属十八个企事业单位技术革新工作情况的检查。一年来,全局广大职工,在毛主席三项
三高炉(210立方米)1963年四季度炉基温度(指炉基1~#孔见图一),曾一度升至325℃±。经过年底封炉10天进行中修后,炉基温度下降至240℃±。但至1964年一季度炉基温度又回升至3
本刊综合消息日前,国家食品药品监督管理局整顿和规范药品市场秩序专项行动工作方案出台,全国各地药品监督管理部门积极部署、落实方案。截至目前,各地已开展了一系列的专项
目前,吉林省1只梅花鹿的价格只卖400元,一些不太好的品种甚至更低,不抵1头猪价,专家认为,这种现象表明价值规律在市场中失灵了,很大部分原因是由人为因素造成的,一些中间商收
1、1971~1975年的钢铁生产从表1可以看出,1971~1975年苏联钢铁生产虽有一些进展,但生铁、钢、钢材、钢管以及铁矿石等主要钢铁产品都没有达到予计的指标,钢铁生产劳动力不足,
我矿选矿厂投产已廿多年,随着社会主义革命和建设的飞速发展,选矿生产和技术经济指标都超过了原设计水平。特别是处理能力已超过原设计的一倍左右。处理能力的扩大,选矿设备
株洲电炉厂革命职工坚持自力更生、艰苦奋斗,于最近试制成功了HX—0.5型新系列炼钢电弧炉。 HX—0.5型新系列炼钢电弧炉是根据73年电炉行业会议的决定和一机部下达的新产品
今年5月15日到21日,广东省冶金局在大宝山矿召开了推广优选法和技术革新经验交流会。参加会议的有99个单位的代表共164人。 会议期间传达了冶金部邯邢现场会议的精神,听了冶