【摘 要】
:
The anodic surface oxidation of natural pyrrhotite in 0.3 mol/L KCl and HCl solution (pH 4. 0) and 0.1 mol/L Na2 B4O7 solution (pH 9.18) respectively was invest
【机 构】
:
SchoolofResourcesProcessingandBioengineering
【出 处】
:
Transactions of Nonferrous Metals Society of China