论文部分内容阅读
<正>Ti6A14V alloy parts were prepared by metal injection molding. Brown parts were densified at 1 200-1 260℃for 2-4 h in vacuum atmosphere. The as-sintered specimens were treated through Hot-Isostatic Pressure(HIP) at 960℃and 140 MPa. Ti6A14V alloy c