The WO3/C composite was successfully prepared by calcination of a mixture of WO3 and g-C3N4 at 520 oC. The as-synthesized samples were analyzed by X-ray diffraction (XRD), electronic differential system (EDS), scanning electron microscopy (SEM), infrared