以FX-501改性酚醛玻璃纤维塑料模压成形的塑压件,由于模具表面局部光洁度差,零件形状复杂等原因,在起模后会发现尖角、圆角、棱边以至平面的局部处有缺边、崩落和凹坑等小缺陷,可以用如下方法修复: 先将缺陷处清理干净,再把和塑压件材质相同的废品件磨削成粉末,用501胶水搅成糊状。快速将糊状物涂在缺陷处,并略高出表面少许。待完全干固之后,使用锉刀精心修理,以达到图纸要求。修完后,即用于布将表面擦干净。
With FX-501 modified phenolic fiberglass plastic molding plastic parts, due to poor surface finish of the mold surface, the shape of complex parts and other reasons, will be found after the sharp corners, rounded corners, edges and even the local at Lack of edge, avalanches and pits and other small defects, you can use the following methods to repair: First clean defects, and then the same pieces of plastic materials and pieces of the same grinding into powder, with 501 glue stir into a paste. Apply the paste to the defect quickly and slightly above the surface. To be completely dry, the use of file carefully repaired in order to achieve the requirements of the drawings. After repair, that is, for the cloth to wipe the surface clean.