Sn(OH)4 was prepared by the conventional solution precipitate method,followed by supercritical CO2 drying.The resultant Sn(OH)4 was divided into three aliquots and calcined at 400,600 and 800 °C,respectively,thus SnO2 nanoparticles with average cryst