【摘 要】
:
零件损坏处的焊前准备和设备裂纹裂纹焊前准备包括:裂纹区的修理和开坡口。零件应放在平台上,使裂纹处在水平平面内。在可接近处沿全裂纹长度铲坡口,并用厚度不大于6~7毫米的
论文部分内容阅读
零件损坏处的焊前准备和设备裂纹裂纹焊前准备包括:裂纹区的修理和开坡口。零件应放在平台上,使裂纹处在水平平面内。在可接近处沿全裂纹长度铲坡口,并用厚度不大于6~7毫米的砂轮修整。在难于铲割之处,应用刮刀、尖头凿子等处置。坡口尺寸取决于指定之处的壁厚。铝合金零件裂纹的端部不要钻孔,因多次加热不会使裂纹加长。
Pre-weld preparation and equipment crack at parts damage Pre-weld preparation includes: repair of cracked areas and beveling. Parts should be placed on the platform so that the crack is in a horizontal plane. Grooves shall be made along the full crack length in accessible areas and trimmed with a wheel of not more than 6 to 7 mm in thickness. Difficult to shovel cut where the use of scrapers, pointed chisel and other disposal. The groove size depends on the wall thickness specified. Aluminum alloy parts do not crack the end of the hole, due to repeated heating will not make the crack longer.
其他文献
目前,关于石油钻机动力传动机组柴油机与变矩器的最佳匹配问题,国内研究甚少。据悉,美国国民供应公司的C型变矩器现有16种规格,可满足各种柴油机的匹配需要。本文根据对C型
索尔斯克钼公司汽车运输车间有100多辆自卸汽车.在整个生产费用中运输费用占37%,所以该公司主要任务之一就是合理地组织大载重量生产汽车的运输。完成第十个五年计划的重要条
用混合表面活性剂制备柴油──水微乳液PREPARATIONOFDIESEL-WATERMICROEMULSIONFROMMIXINGSUREACTANT范绮莲,李蒙俊,邹红林1前言燃油掺水形成乳化液,使燃烧更加完全,从而提高燃烧率及减少废气对环境的污...
PREPARATION OF DIESEL WITH HYBR
用大口径毛细管柱气相色谱 /电子捕获器 (GC/ECD)方法测定新鲜荔枝中“六六六”4种异构体的农药残留 10min即可把 4种异构体有效分离检测 α BHC ,β BHC ,γ BHC ,δ BHC
Forest growth is mainly currently monitored using in-situ measurements in northeast of China.To effectively monitor forest growth disturbance at large scale,we
A multi-quantum barrier structure is employed as the electron blocking layer of light-emitting diodes to enhance their performance.Using the non-isothermal mult
首次采用共振光散射、荧光光谱并结合平衡透析法研究了 I- 与人血清白蛋白 ( human serum albumin,简称 HSA)或牛血清白蛋白 ( Bovine Serum Albumin,简称 BSA)结合平衡。首
(一)什么是液压-机械拉延液压-机械拉延是一种将金属平板或预成形的金属板变为圆柱形、棱柱形、圆锥形或抛物线形空心体的深拉延方法。被加工的盘状毛坯直接受到压力可调的
这些要求归纳起来,包括下述三个方面:1.火花塞上适当的点火参数:适当的火花能量,适当的点火电压,较快的二次电压上升时间(火花塞上的电压从峰值的10%到90%所需的时间)。
汽车运输科学研究院列宁格勒分院于1971年提出了环氧树脂的配方和修复工艺,它是采用各种校正方法来修复“吉尔”——164发动机气缸体主轴承轴瓦座。该工艺的特点是用校正工