采用手工电弧焊修复锻模的方法

来源 :机械工人 | 被引量 : 0次 | 上传用户:loveshdou
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
我们车间两吨锤使用的锻模从中间开裂了,新的锻模还没有投入生产,即使新锻模投入生产后,也得几个月时间才能生产出来。这样不仅影响了当月生产任务,而且还会影响到全年生产任务的完成。因此,修复好锻模就成为当务之急。修复的锻模。锻模裂纹产生在燕尾根部,是一条贯穿裂纹,从F面观察,可以看到宽度为2毫米、深为100毫米的裂纹。从F~1 The forging dies used on the two-ton hammer in our workshop were cracked in the middle, and the new forging dies were not yet in production. Even after the new forging dies were put into production, they had to be produced for several months. This not only affected the production tasks of the month, but also affect the completion of the annual production tasks. Therefore, repairing a forging die becomes a top priority. Repair forging die. Forging die cracks in the dovetail root, is a through cracks, viewed from the F surface, you can see the width of 2 mm, 100 mm deep crack. From F ~ 1
其他文献
我们成功地研制了一种加速零件渗碳的固体渗碳剂。其配方为:每70克苏打粉(Na_2CO_3)和亚铁氰化钾(黄血盐K_4〔Fe.(CN)_6〕·3H_2O)加1公斤木屑配制而成,拌合均匀后即可使用
请下载后查看,本文暂不支持在线获取查看简介。 Please download to view, this article does not support online access to view profile.
1.试验条件: 采用NBC—400硅整流平特性电源空载电压20~64伏(可调),额定焊接电流400安,工作电压18~45伏。将MZP—1000型控制箱和MZT—1000型焊车改进后,组装为自动焊机。气路
广西壮族自治区素有“八山一水一分田”之称,国有林场历来是广西林业的重要组成部分,在区生态环境和林业产业建设中具有“半壁江山”的地位。全区现有国有林场151个,其中中直1个、自
目的探讨雷公藤多苷联合替米沙坦治疗糖尿病肾病的临床疗效。方法选取2012年10月—2014年10月天津市第一中心医院内分泌科收治的2型糖尿病肾病患者126例,随机分为对照组(64例)
碳、硅、锰、硫、磷五种元素的含量对铸件性能有很大的影响。但是,目前许多工厂配料时,一般只考虑一、两种元素如碳、硅或碳、锰,随后再加锰铁和硅铁调整,至于对硫、磷元素
在螺纹磨床上加工螺距(t)在0.5mm以下的螺纹时,因为螺距小,要求齿底平面的宽度一般在0.05mm以下(图1)。由于砂轮不易修尖,或者是虽修尖但在加工中不易保持,结果是很难磨出合
导布辊在印染机械中应用最多,批量较大。它主要用来控制织物的行进方向。其表面要求耐腐蚀;辊体要求具有一定的刚度;其运动方面有较严格的静平衡要求。我厂φ125×2800宽幅
经济专家预测,我国消费市场第三次浪潮已经开始。这次“浪潮”的特点是:提高生活质量、实现消费现代化。这次“浪潮”的冲击点将是:录像机、摄像机、空调机、电话、现代厨房
一、前言我厂在研制某产品中,为解决散热问题,设计上采用了结构紧凑,换热效率高的板翅式换热器新技术。但这种板翅式换热器要达到预想效果必须设计一种重量轻、强度高、形状