The anodic overvoltage of the carbon anode in aluminum electrolysis isof the order of 0.6 V at normal current densities. However, it can be reduced somewhat by
In order to establish a model between the grain size and the process parameters, the hot deformation behaviors of Ti-49.5Al alloy was investigated by isothermal
Two two-step techniques, called TS2/TS7 and TS3/TS7, respectively, have been developed to form cerium conversion films on the surface of industrial pure aluminu
Ultrafine milling technology is used to treat gold-bearing sulphides and to investigate the effects of minerals size, milling time, liquid/solid ratio, NaCN con
The phase behavior and interfacial tension of alkali/surfactant/polymer (ASP) flooding system and simulative crude oil were investigated, and the size distribut