论文部分内容阅读
POSCO已成功开发一种新型高速轧制工艺 ,该工艺用于生产厚度小于 2 3mm的热轧钢板。POSCO公司预期此工艺通过缩短平均轧制时间 ( 1 0s)可使产量每年增加 2 1万t。浦项厂热轧部门成功解决了诸如 :薄钢板前端在轧制过程中容易产生折叠 ,冷却水会影响穿带速度等
POSCO has successfully developed a new high-speed rolling process for producing hot-rolled steel sheets with a thickness of less than 23 mm. POSCO expects this process to increase output by 210,000 t / year by reducing the average rolling time (10 s). Posco hot-rolled sector successfully resolved such as: the front end of the sheet in the rolling process prone to folding, cooling water will affect the wear speed