鞍钢东烧厂600 mm料层厚度赤精矿烧结工艺参数研究

来源 :中国冶金 | 被引量 : 0次 | 上传用户:abcdewwy
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
为了将鞍钢集团矿业公司东烧厂现有的500 mm烧结料层提高到600 mm,对东烧厂赤铁矿的烧结特点进行分析,以赤铁矿为主要原料进行实验室600 mm厚料层烧结杯试验,研究出获得化学成分稳定、机械强度高、粒度均匀、高温冶金性能优良的烧结矿的最佳工艺参数。为鞍钢东烧厂进一步提高料层厚度提供理论依据。 In order to increase the existing 500 mm sinter bed of the Anshan Iron and Steel Group Dongfang Plant to 600 mm, the sintering characteristics of hematite in Dongfang Iron Ore Plant were analyzed. The hematite was used as the main raw material for the laboratory 600 mm thick bed Sintering cup test, developed to obtain the chemical composition of the stable, high mechanical strength, uniform size, high-temperature metallurgical performance of the best sintered sinter process parameters. For the Anshan Iron and Steel East burning plant to further improve the material thickness to provide a theoretical basis.
其他文献
简介了济钢第一炼钢厂在炉龄提高后的炉型控制状况;重点针对溅渣后炉型的变化,优化了溅渣护炉和砌炉工艺,改进了炉渣性质,进而提高了溅渣护炉效果和保持了合理炉型,保证了生
@@焊接自动化是通过先进的焊接设备,在焊接过程中,利用自动化、智能化的控制系统,实现焊前装配的准确快速装卡,焊接过程的实时监控和焊后产品的质量检测,以实现零件批量化、柔性化
@@2009年是我国实施国民经济和社会发展“十一五”规划的第四年。由于国际金融危机的影响,2009年成为进入新世纪以来我国经济发展最为困难的一年。回顾2009年行业的发展历程,可
通过在热轧四辊可逆粗轧机上使用高铬钢轧辊,大大提高了轧辊耐磨性和使用寿命,降低了轧辊消耗,有效地减少了轧辊热疲劳裂纹以及剥落现象,对作业率和板带产品成材率的提高起到
中文名:艾伦·佩姬英文名:Ellen Page生日:1987年2月21日出生地:加拿大哈利法克斯最新作品:《超级英雄》(Super)(2011年上映)《盗梦空间》(Inception)(2010年9月1日上映)当20
为了培养钢结构行业创新性人才,浙江树人大学于2008年在城建学院设立土木工程专业钢结构方向创新实验班。实验班注重学生创新能力的培养,同时加强学生接触实际工程和动手能力的
会议
快速发展的钢结构行业对钢结构应用型人才需求激增,而现有的专业方向设置及人才培养模式不能满足这一要求,通过对钢结构行业的调研,设置了钢结构专业培养方向。并通过课程设置、
介绍了莱钢120 t转炉副枪的应用情况,莱钢炼钢厂通过不断优化数学模型和完善修改各项规程制度使副枪运行得到了稳定,基本上取消了转炉倒炉作业,并对转炉炼钢工艺操作进行了优
针对目前我校钢结构课程设计存在的问题,采用教学改革试点,结合近几年教学与课程设计指导实践经验,从课程设计内容的优化组合、设计题目多样化、设计过程管理指导、完善课程设计
本文结合了土木工程专业系列课程的设计实践,提出应把各主要专业课的设计以一个设计方案连贯起来,并进行系统化、整体化的教学指导,从而提高专业设计的质量,培养学生的综合能力。