在钢坯的连续铸造中,使铸坯内部的液芯停止在铸坯拉坯轧迹的特点Q处,在该Q点的下流侧形成空芯,在铸坯拉坯行程的后半部用轧辊将空芯部压接轧制,制成实心铸坯。通过采用适当的浇铸温度得到的实心铸坯由外皮激冷细晶和内部的柱状晶构成。另外还公开了将连铸与后续热轧工序结合起来的钢材连铸连轧方法。据此可以获得铸造效率的飞跃提高、质量的改善和铸造壁厚自由的铸坯设备,并且能够将连铸与轧制直接连结,使各种钢材接近于制品 In the continuous casting of a billet, the liquid core in the billet is stopped at the characteristic Q of the billet bloom, the hollow core is formed on the downstream side of the point Q, and the nip is formed by the nip The hollow core is crimped and rolled to a solid slab. The solid slab, obtained by using a suitable casting temperature, is composed of a chilled fine crystal of the skin and an internal columnar crystal. In addition, the continuous casting and rolling process of continuous casting and subsequent hot rolling are also disclosed. Accordingly, it is possible to improve the casting efficiency, improve the quality, and to cast a strand slab having a free wall thickness, and to connect the continuous casting and the rolling directly so as to bring the various types of steel close to the product
其他文献
广东省政府办公厅日前印发《关于加快推进我省云计算发展的意见》,《意见》提出,到2015年广东省云计算产业产值要超千亿元,并培育10家左右云计算龙头企业及一批创新能力强的
1 前言高还原性烧结矿是高炉冶炼的理想精料。随着600mm料层低温烧结工艺的实现,在二烧50m~2烧结机上生产高还原性烧结矿的时机已经成熟。1999年3月开始,在碱度不提高的条件
本文描述连铸过程中水口堵塞的类型及特征,分析了水口堵塞的成因,提出防止水口堵塞的措施。 This article describes the types and features of nozzle clogging during co
日本 NKK公司京滨厂过去采用铸锭—开坯工艺生产无缝钢管及条钢用的3 30 mm大断面圆坯。最近 ,为了降低坯料成本 ,提高产品成材率 ,对该厂的 5号连铸机 (圆坯连铸机 )进行
在实验的基础上 ,对氧化气氛下铜的氯化机理进行了研究 ,实验结果证明了铜在氧化气氛下的氯化历程 ,其机理为以O2 为催化剂的循环催化反应 ,并获得了以下动力学参数 :表观反
夏季到来,减肥又成为爱美人士关心的话题,减肥的方式有很多种,减肥茶是很多“懒人”首选的,不运动,不节食,喝喝茶,就可以消肥了,特别是碧生源减肥茶,因为强大的广告攻势,博得
不锈钢的高氮化不仅可提高钢的耐蚀性 ,而且可促进奥氏体相的稳定化和取代贵金属 Ni,从而达到产品品质与成本方面的双收益 ,然而 ,高氮不锈钢的生产必须在加压气氛下进行。目
模型概观一文进行了渣 -铁平衡及液相流动计算的模型研究 ,预测并改进了钢中夹杂物的组成。在模拟参数的优化方面 ,提供准确的化学数据至关重要。本文论述了如何应用各种化学
通过对 4 88例原诊断为甲状腺腺瘤的病理资料进行复查、回顾性分析 ,发现其中仅 5 6%为真正的腺瘤 ,其余的 4 4 %为单结节性甲状腺肿 .认为过去对腺瘤诊断过松 ,应严格按照腺