浙江检验出鞋类产品帮底脱胶致返工延误出口

来源 :中国皮革 | 被引量 : 0次 | 上传用户:xuzhidanxu
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
前不久,浙江温州检验检疫局工作人员在现场检验出口鞋类产品时,连续发现两家企业的3批、232箱、3130双PU胶粘鞋因帮底脱胶导致返工整理而延误了出口。脱胶主要原因是帮底粘合强度不符要求。据了解,帮底粘合强度是影响鞋子穿用时最主要的物理耐用性能之一。按照鞋类检验规程SN/T1932.2-2010要求,皮鞋的帮底粘合强度须满足每毫米不小于2牛顿的力。今年上半年的实验室统计数据显示,帮底粘合强度不合格占抽样皮鞋不合格原因的55%。据分析,在酷暑天气条件下,脱胶 Not long ago, Wenzhou, Zhejiang Inspection and Quarantine staff at the scene to test the export of footwear products, found two batches of 3 batches of enterprises, 232 boxes, 3130 pairs of PU adhesive shoes due to the bottom degumming led to rework and delay the export. The main reason for degumming is to help the bottom adhesive strength does not match the requirements. It is understood that the bottom bonding strength is one of the most important physical durability of shoes. In accordance with the footwear inspection procedures SN / T1932.2-2010 requirements, the adhesive strength of the shoes to the bottom to meet the force of not less than 2 Newtons per millimeter. The first half of this year’s laboratory statistics show that the end of the bonding strength of substandard shoes accounted for 55% of the reasons failed. According to the analysis, in the summer weather conditions, degumming
其他文献
按ISO9000系列国际标准要求健全质量体系;阐述研究所单件、小批量、多品种特点条件下健全质量体系的指导思想及方法。
简要介绍了在研的德国国家级材料研究计划MeTech的背景情况及部分项目计划.它山之石,可以攻玉.目的是通过介绍德国的材料研究计划,促进我国的十五计划的制定和落实.
我从1975年从事专职新闻工作,迄今已有15个春秋。这15年,在市以上新闻单位发表的作品。每年都在一百篇以上。许多同行对我的用稿量感到惊讶。其实,我并无什么大的本事,只是
混凝土路面病害的种类及成因分析,判定与检测手段及对其利用方式.
该文就改革开放新形势下,围绕知识创新培养目标营造新的培养模式问题进行了探讨,并提出了实施的新思路。