摘要:随着我国高层建筑的逐渐增多,大体积混凝土的浇筑、超高层的建筑的实施,高层建筑的质量隐患也越来越得到人们的重视,特别是现浇的混凝土结构其表面裂缝更是最为突出。虽然是不会影响整体建筑质量的隐患,但是感观质量的存在也较为突出。本文从高层建筑较易出现的大体积混凝土裂缝、楼板裂缝的出现原因及改进措施给予分析。
关键词:高层建筑、质量隐患、沉降、裂缝
Abstract: along with the high-rise building increases gradually, of mass concrete casting, the implementation of the construction of the tall, the quality of the high-rise buildings hidden trouble also more and more get the attention of people, especially the cast-in-situ concrete structure its surface crack is the most outstanding. Although it is will not affect overall building quality hidden trouble, but the existence of the sensory quality also is serious. This paper, from the high-rise buildings appear more easily to the mass concrete crack, floor occurrence of crack reasons and improvement measures to analysis.
Keywords: high building, quality hidden trouble, settlement, crack
中图分类号:[TU208.3]文献标识码:A 文章编号:
前言:高层建筑在设计中已经保证了其承载能力极限状态,虽然在设计中对正常使用状态有些许考虑,但是根据不同的施工工艺及施工个人,真正的不可确定性因素较难把握。所以以下就其高层建筑在施工过程中宜出现的问题总结如下:
1.大体积混凝土裂缝:
高层建筑及地下车库的普遍使用,大体积混凝土的浇筑也随即出现,对于大体积混凝土最为常见的即为裂缝。混凝土浇筑后,由于混凝土的导热性能低混凝土体积大,在内部水化热不易散发,混凝土表面散热快,内部温升高,形成内外温差,产生温度应力,容易产生表面裂缝。按国内外经验,只要控制砼内外温差不大于30℃,即可防止表面裂缝。因温度升高而发生的第二种裂缝是收缩裂缝。混凝土降温引起砼硬化收缩,但混凝土变形受基底灰色淤泥质粘土和大直径钻孔灌注桩的约束使砼底板发生应力,经验算,该基础底板产生的拉应力小于混凝土的抗拉强度,基础底板不会由于降温差和混凝土收缩而引起收缩裂缝。
1.1确定方法
混凝土浇筑必须保证连续性,按照“一个坡度、循环推进、分批浇筑”的方法进行浇筑,保证底板一次性连续浇筑。每段浇筑长度控制在2-3米,做到逐段呈梯形向前推进。精确计算车辆的运行时间,浇筑时间,做到时间占满、空间占满。
1.2混凝土的浇筑
在浇筑混凝土时,分层振捣以使混凝土的水化热尽快散失,其次采用二次振捣的方法,增加混凝土的密实度,提高抗裂能力,振捣时间控制在10-30秒,以混凝土开始泛浆和不冒气泡为准。为防止收缩裂缝我们采取了二次抹压措施,混凝土终凝前,排除表面泌水,木杠刮平,采用木抹子拍打密實,再次抹平,消除了因泌水及早期收缩产生的裂缝。
1.3混凝土的测温
采用热电偶进行跟踪测温,共设置53个测温点,每点设上、中、下三个测温部位,在砼浇筑完3-5天内温度达到峰值,5天后温度开始下降,在上升阶段每2小时测一次,下降阶段每8小时测一次。测温的主要内容为:大气温度及砼内部温度、上表面温度、入模温度,各种测温及时记录,并计算温差以便调整养护。
1.4混凝土的养护:
底板大体积混凝土养护是混凝土质量保证的关键步骤,为了保证新浇混凝土有适宜的硬化条件,防止早期由于干缩而产生的裂缝,大体积混凝土浇筑完毕后,加以塑料薄膜及双层麻袋覆盖(既保温又隔热作用)养护,根据计算和实测温差随时调整冷凝水管中的流水速度,将温差控制在25℃规范以内。
2.现浇楼板裂缝的控制:
2.1从住宅工程现浇楼板裂缝发生的部位分析,最常见、最普遍和数量最多的是房屋四周阳角处(含平面形状突变的凹口房屋阳角处)的房间在离开阳角1米左右,即在楼板的分离式配筋的负弯矩筋以及角部放射筋未端或外侧发生45度左右的楼地面斜角裂缝,此通病在现浇楼板的任何一种类型的建筑中都普遍存在.。其原因主要是砼的收缩特性和温差双重作用所引起的,并且越靠近屋面处的楼层裂缝往往越大。
2.2从设计角度看,现行设计规范侧重于按强度考虑,未充分按温差和混凝土收缩特性等多种因素作综合考虑,配筋量因而达不到要求.而房屋的四周阳角由于受到纵、横二个方向剪力墙或刚度相对较大的楼面梁约束,限制了楼面板砼的自由变形,因此在温差和砼收缩变化时,板面在配筋薄弱处(即在分离式配筋的负弯矩筋和放射筋的未端结束处)首先开裂,产生45度左右的斜角裂缝.虽然楼地面斜角裂缝对结构安全使用没有影响,但在有水源等特殊情况下会发生渗漏缺陷,容易引起住户投诉,是裂缝防治的重点。
2.3商品砼的性能改善:选用质量可靠地商品混凝土也是尽量避免出现裂缝的方法之一。2.4施工中应采取的主要技术措施 :
(1).严格控制混凝土施工配合比。严格控制水灰和水泥用量。选择级配良好的石子,减小、空隙率和砂率以减少收缩量,提高混凝土抗裂强度。
(2)在混凝土浇捣前,应先将基层和模板浇水湿透,避免过多吸收水分。浇捣过程中应尽量做到既振捣充分又避免过度。在楼板浇捣过程中更要派专人护筋,避免踩弯面负筋的现象发生。通过在大梁两侧的面层内配置通长的钢筋网片,承受支座负弯矩,避免因不均匀沉降而产生的裂缝。
(3)混凝土楼板浇注完毕后,表面刮抹应限制到最小程度,防止在混凝土表面撒干水泥刮抹,并加强混凝土早期养护。楼板浇注后,对板面应及时用材料覆盖、保温,认真养护,防止强风和烈日曝晒。
(4)施工后浇带的施工应认真领会设计意图,制定施工方案,杜绝在后浇处出现混凝土不密实、不按图纸要求留企口缝以及施工中钢筋被踩弯等现象。同时,更要避免在未浇注混凝土前就将部分模板、支柱拆除而导致梁板形成悬臂,从而造成变形等现象的发生。浇注后,当楼板出现裂缝面积较大时,应对楼板进行静载试验,检验其结构安全性,必要时可在楼板上增做一层钢筋网片,以提高板的整体性。
(5)严格施工管理,浇捣楼板混凝土时,必须铺设操作平台,防止施工操作人员直接踩踏上皮负弯矩钢筋。同时加强浇捣楼板混凝土整个过程中的钢筋看护,随时将位置不正确的钢筋复位,确保其位置准确。
以上几种方法由于受到不同条件的限制,故应以提高楼板含钢率为主,并可以有针对性地在外墙转角楼板处增配放射性配筋,提高部分外墙的保温隔热标准。特别是对外墙转角处的里墙面,要采用加贴保温隔热材料的办法,使温差对楼板变形带来的影响,减少到最低限度。
结语:虽然现浇混凝土裂缝的出现是不可避免的但是在施工过程中,还要适当地施工速度,严格施工操作程序,不盲目赶工。杜绝过早上传、上荷载和过早拆模。做到科学施工,坚决摒弃违反科学的蛮干的做法。只有这样,才能使当前民用建筑楼板结构裂缝的这一质量顽症得到有效遏制。
参考文献
[1]王铁梦、工程结构裂缝控制.北京:中国建筑业出版社,
[2]牛紫龙,混凝土施工中温度裂缝的分析与控制,工程建设,
[3]朱伯芳.大体积混凝土温度应力与温度控制,中国电力出版社,
[4]梁博顺.大体积混凝土筏板基础施工技术探析.中华建设,
关键词:高层建筑、质量隐患、沉降、裂缝
Abstract: along with the high-rise building increases gradually, of mass concrete casting, the implementation of the construction of the tall, the quality of the high-rise buildings hidden trouble also more and more get the attention of people, especially the cast-in-situ concrete structure its surface crack is the most outstanding. Although it is will not affect overall building quality hidden trouble, but the existence of the sensory quality also is serious. This paper, from the high-rise buildings appear more easily to the mass concrete crack, floor occurrence of crack reasons and improvement measures to analysis.
Keywords: high building, quality hidden trouble, settlement, crack
中图分类号:[TU208.3]文献标识码:A 文章编号:
前言:高层建筑在设计中已经保证了其承载能力极限状态,虽然在设计中对正常使用状态有些许考虑,但是根据不同的施工工艺及施工个人,真正的不可确定性因素较难把握。所以以下就其高层建筑在施工过程中宜出现的问题总结如下:
1.大体积混凝土裂缝:
高层建筑及地下车库的普遍使用,大体积混凝土的浇筑也随即出现,对于大体积混凝土最为常见的即为裂缝。混凝土浇筑后,由于混凝土的导热性能低混凝土体积大,在内部水化热不易散发,混凝土表面散热快,内部温升高,形成内外温差,产生温度应力,容易产生表面裂缝。按国内外经验,只要控制砼内外温差不大于30℃,即可防止表面裂缝。因温度升高而发生的第二种裂缝是收缩裂缝。混凝土降温引起砼硬化收缩,但混凝土变形受基底灰色淤泥质粘土和大直径钻孔灌注桩的约束使砼底板发生应力,经验算,该基础底板产生的拉应力小于混凝土的抗拉强度,基础底板不会由于降温差和混凝土收缩而引起收缩裂缝。
1.1确定方法
混凝土浇筑必须保证连续性,按照“一个坡度、循环推进、分批浇筑”的方法进行浇筑,保证底板一次性连续浇筑。每段浇筑长度控制在2-3米,做到逐段呈梯形向前推进。精确计算车辆的运行时间,浇筑时间,做到时间占满、空间占满。
1.2混凝土的浇筑
在浇筑混凝土时,分层振捣以使混凝土的水化热尽快散失,其次采用二次振捣的方法,增加混凝土的密实度,提高抗裂能力,振捣时间控制在10-30秒,以混凝土开始泛浆和不冒气泡为准。为防止收缩裂缝我们采取了二次抹压措施,混凝土终凝前,排除表面泌水,木杠刮平,采用木抹子拍打密實,再次抹平,消除了因泌水及早期收缩产生的裂缝。
1.3混凝土的测温
采用热电偶进行跟踪测温,共设置53个测温点,每点设上、中、下三个测温部位,在砼浇筑完3-5天内温度达到峰值,5天后温度开始下降,在上升阶段每2小时测一次,下降阶段每8小时测一次。测温的主要内容为:大气温度及砼内部温度、上表面温度、入模温度,各种测温及时记录,并计算温差以便调整养护。
1.4混凝土的养护:
底板大体积混凝土养护是混凝土质量保证的关键步骤,为了保证新浇混凝土有适宜的硬化条件,防止早期由于干缩而产生的裂缝,大体积混凝土浇筑完毕后,加以塑料薄膜及双层麻袋覆盖(既保温又隔热作用)养护,根据计算和实测温差随时调整冷凝水管中的流水速度,将温差控制在25℃规范以内。
2.现浇楼板裂缝的控制:
2.1从住宅工程现浇楼板裂缝发生的部位分析,最常见、最普遍和数量最多的是房屋四周阳角处(含平面形状突变的凹口房屋阳角处)的房间在离开阳角1米左右,即在楼板的分离式配筋的负弯矩筋以及角部放射筋未端或外侧发生45度左右的楼地面斜角裂缝,此通病在现浇楼板的任何一种类型的建筑中都普遍存在.。其原因主要是砼的收缩特性和温差双重作用所引起的,并且越靠近屋面处的楼层裂缝往往越大。
2.2从设计角度看,现行设计规范侧重于按强度考虑,未充分按温差和混凝土收缩特性等多种因素作综合考虑,配筋量因而达不到要求.而房屋的四周阳角由于受到纵、横二个方向剪力墙或刚度相对较大的楼面梁约束,限制了楼面板砼的自由变形,因此在温差和砼收缩变化时,板面在配筋薄弱处(即在分离式配筋的负弯矩筋和放射筋的未端结束处)首先开裂,产生45度左右的斜角裂缝.虽然楼地面斜角裂缝对结构安全使用没有影响,但在有水源等特殊情况下会发生渗漏缺陷,容易引起住户投诉,是裂缝防治的重点。
2.3商品砼的性能改善:选用质量可靠地商品混凝土也是尽量避免出现裂缝的方法之一。2.4施工中应采取的主要技术措施 :
(1).严格控制混凝土施工配合比。严格控制水灰和水泥用量。选择级配良好的石子,减小、空隙率和砂率以减少收缩量,提高混凝土抗裂强度。
(2)在混凝土浇捣前,应先将基层和模板浇水湿透,避免过多吸收水分。浇捣过程中应尽量做到既振捣充分又避免过度。在楼板浇捣过程中更要派专人护筋,避免踩弯面负筋的现象发生。通过在大梁两侧的面层内配置通长的钢筋网片,承受支座负弯矩,避免因不均匀沉降而产生的裂缝。
(3)混凝土楼板浇注完毕后,表面刮抹应限制到最小程度,防止在混凝土表面撒干水泥刮抹,并加强混凝土早期养护。楼板浇注后,对板面应及时用材料覆盖、保温,认真养护,防止强风和烈日曝晒。
(4)施工后浇带的施工应认真领会设计意图,制定施工方案,杜绝在后浇处出现混凝土不密实、不按图纸要求留企口缝以及施工中钢筋被踩弯等现象。同时,更要避免在未浇注混凝土前就将部分模板、支柱拆除而导致梁板形成悬臂,从而造成变形等现象的发生。浇注后,当楼板出现裂缝面积较大时,应对楼板进行静载试验,检验其结构安全性,必要时可在楼板上增做一层钢筋网片,以提高板的整体性。
(5)严格施工管理,浇捣楼板混凝土时,必须铺设操作平台,防止施工操作人员直接踩踏上皮负弯矩钢筋。同时加强浇捣楼板混凝土整个过程中的钢筋看护,随时将位置不正确的钢筋复位,确保其位置准确。
以上几种方法由于受到不同条件的限制,故应以提高楼板含钢率为主,并可以有针对性地在外墙转角楼板处增配放射性配筋,提高部分外墙的保温隔热标准。特别是对外墙转角处的里墙面,要采用加贴保温隔热材料的办法,使温差对楼板变形带来的影响,减少到最低限度。
结语:虽然现浇混凝土裂缝的出现是不可避免的但是在施工过程中,还要适当地施工速度,严格施工操作程序,不盲目赶工。杜绝过早上传、上荷载和过早拆模。做到科学施工,坚决摒弃违反科学的蛮干的做法。只有这样,才能使当前民用建筑楼板结构裂缝的这一质量顽症得到有效遏制。