7月1日,从有关部门获悉,巨化氟化公司顺利领到了《一种2,3,3,3-四氟丙烯的制备方法》美国专利证书,这是巨化通过PCT国际专利申请获得的首个国际专利。目前国际条约和欧美发达国家新出台法规,第3代氟制冷剂的淘汰政策越来越明朗,产品的生存空间逐渐被挤压,国际氟化工巨头对第4代氟制冷剂的技术限制和专利壁垒 July 1, learned from the authorities, Juhua Fluoride successfully received the “a 2,3,3,3-tetrafluoropropene preparation method,” the United States patent certificate, which is a huge PCT international patent applications obtained The first international patent. The current international treaties and developed countries in Europe and the United States introduced the new regulations, the third generation of fluorine refrigerant phase-out policy is becoming clearer and clearer, the living space of products is gradually being squeezed, the international fluorine chemical giant on the 4th generation fluorine refrigerant technical limitations and patents barrier
其他文献
针对重力铸造的汽车活塞用单一SiC颗粒增强铝基复合材料拉伸性能会降低的问题,采用混合盐原位反应的方法制备出综合力学性能较好的TiB2、SiC双相颗粒增强的ZL101复合材料。利
为了让广大读者能及时了解我国汽车新产品上市情况,本刊编辑部今后将及时刊登国家发改委的新产品公告 根据原国家经贸委《关于车辆生产企业及产品目录管理改革有关问题的通
期刊
采用自制的雾化-激冷设备,用快速凝固粉末冶金方法制备了Si增强AZ91镁基复合材料,分别对材料进行光学金相、XRD、显微硬度、拉伸性能以及SEM分析。结果表明:增强相在基体中分布均匀,在挤压过程中增强相与基体发生了反应,形成反应层,反应层中存在高温相Mg2Si。复合材料的室温δ、σb、σ0.2分别为3.50%、322.35 MPa和241.60 MPa。随着Si含量的提高,该复合材料的性能明显下降
目的 观察止痉散贴敷治疗小儿高热惊厥的临床疗效.方法 62例高热惊厥患儿随机分成两组,对照组30例予常规西医治疗,治疗组32例加予止痉散贴敷涌泉穴,疗程均为3d.结果 治疗组退
目的 分析混合外固定治疗C2、C3型Pilon骨折的临床价值.方法 2004年9月至2009年9月,采用混合外固定治疗C2、C3型Pilon骨折21例.结果 所有患者获得随访,随访时间1~2年,平均1.3
期刊
采用激光表面处理的方法,优化激光工艺参数,对激光改性表面的冷凝换热特性进行了实验比较研究。发现了激光表面改性换热管促进了滴状冷凝形态特性,提高了凝结换热系数;通过对
以30~54μm的二硅化钼为喷涂粉末,研究了喷涂参数对二硅化钼涂层微观结构的影响。结果表明,喷涂过程中,喷涂粉末中部分四方相MoSi2(t)转变为六方相MoSi2(h),MoSi2中Si含量出现