1992年10月,我部在配合武陵开发区基建工程中,发现一座东汉烧砖窑址,并进行发掘。砖窑开挖于生土层中。据调查,此地原为一小山岗,70年代造田时被推为平地,耕地层下即为窑址。 (一)砖窑结构窑址除顶部塌陷损坏外,保存基本完好(图一)。窑长4.7、宽2.3米,方向260°。 1.操作坑系窑门外与窑相连的土坑,坑的一边被一现代水沟破坏。坑底由外向窑门倾斜呈一缓坡,靠近窑门处堆有大量草木灰。 2.窑体砖窑由窑门、火膛、窑床三部分构成,火膛近半圆形,窑床近长方形(图
In October 1992, in coordination with the infrastructure project in Wuling Development Zone, the Ministry of Foreign Affairs found an East Han Dynasty burned brick kiln and excavated it. Brick excavation in the soil layer. According to the survey, the place was originally a small hill. In the 1970s, it was pushed to the ground when the farmland was constructed. (A) In addition to the top of the brick kiln structure cave damage, the preservation of basic intact (Figure 1). Kiln length 4.7, width 2.3 meters, the direction of 260 °. 1. Operation Pit Hanging from the kiln outside the kiln pit, one side of the pit was destroyed by a modern ditch. Bottom from the outward tilt of the kiln door was a gentle slope, near the kiln door at a large pile of ash. 2. Kiln kiln The kiln door, fire bore, kiln bed is composed of three parts, the fire chamber nearly semi-circular kiln bed nearly rectangular (Figure