论文部分内容阅读
第一册大会发言:抗非均匀腐蚀的斗争;腐蚀实际损失的估计。A:坦讨论会:高温腐蚀(中心发育) 高温腐蚀当前问题的探讨:Na_2SO_4诱发热腐蚀的电化学研究;几种含钯的镍基超级合金的热腐蚀行为;纯氧中Fe—Al—Mn合金的氧化;氯化物/硫酸盐环境中表面氧化皮对碳钢的影响;激光熔融的不锈钢表面的高温氧化行为;含硫气氛中镍基合金上铝化物层的劣化;运行设备中试样的氢侵蚀。
Volume I General Assembly Address: The fight against non-uniform erosion; Corrosion Actual estimates of losses. A: Tan discussion: high temperature corrosion (center development) of high temperature corrosion current issues: Na_2SO_4 induced hot corrosion electrochemical studies; several palladium-containing nickel-based superalloys corrosion behavior; pure oxygen Fe-Al-Mn The oxidation of the alloy; the effect of the surface scale on the carbon steel in the chloride / sulphate environment; the high temperature oxidation behavior of the laser-melted stainless steel surface; the deterioration of the aluminide layer on the nickel- Hydrogen erosion.