1.高岭土纤维增强硅酸钙板的制造方法《CN1139085A》原材料配方(wt%):石棉12~24;玻纤0~3.5;纸浆0~3.5;钙质材料(其中CaO含量60%~70%)15~25;硅质材料50~70其中合高岭土60~100石英砂或瓷土0~40。原材料经制浆、抄取成型、蒸压养护后制成成品。采用高岭土
1. Method for producing kaolin fiber reinforced calcium silicate board “CN1139085A” Raw material formula (wt%): asbestos 12-24; glass fiber 0-3.5; pulp 0-3.5; calcium material (wherein the CaO content is 60% 70%) 15 ~ 25; siliceous material 50 ~ 70, wherein the combined kaolin clay 60 ~ 100 or 0 ~ 40 clay. Pulp raw materials, copy molding, autoclaved finished products. Using kaolin