In order to produce the fully equiaxed and fine grained pure Al, a simple casting process that used cooling slope was examined and compared with conventional ca
NiTi alloy is produced by mechanical alloying(MA). It becomes amorphous after milling for enough time, such as 100 h in this paper. DSC measurement shows that t
The performances of gradient thermal barrier coatings (GTBCs)produced by EB-PVD were evaluated by isothermal oxidation and cyclic hot corrosion(HTHC) tests.Comp
T he change of microstructure with strain was investigated in a Fe-32Mn-5Si austenitic alloy at room temperature by X-raydiffraction profile analysis. The exper
The width and spacing of adiabatic shear bands (ASBs) in the serrated chips generated during high speed orthogonal cutting of 30CrNi3MoV structural steel were m