To upgrade residual oil, the residual oil was subjected to ultrasonic treatment with an output of 800 W, at a temperature of 70 °C and at intervals ranging
The polypropylene (PP) nanocomposites filled with pretreated halloysite nanotubes (HNTs) were prepared by the melt-blending method. Before filling, the as-recei