采用红外光谱测定了不同催化体系BR及其分级样的微观结构,结果表明,同类催化体系BR及其分级样的微观结构含量基本相同,但不同催化体系的BR则有差异。稀土BR经辐照不发生微观结构变化,其顺式-1,4含量比Ni系略高。实验指出,不同催化剂体系BR的微观结构不受其分子量和支化度的影响。用GPC-自动粘度计联用法的数据计算表明,稀土BR不产生支化,3,4-聚异戊二烯及1,2-聚丁二烯不易产生支化,而Co,Ti,Ni系BR易产生支化。 The microstructure of BR and its graded samples were measured by FTIR spectroscopy. The results showed that the microstructure of BR and its graded samples were basically the same, but the BRs of different catalytic systems were different. Rare earth BR irradiation did not occur microstructure changes, the cis-1,4 content slightly higher than the Ni system. Experiments show that the microstructure of different catalyst system BR is not affected by its molecular weight and degree of branching. Calculated by GPC - automatic viscometer combined data show that BR does not produce branching, 3,4-polyisoprene and 1,2-polybutadiene is not easy to produce branching, and Co, Ti, Ni BR easy to produce branching.
其他文献
本文用动态法研究了D380大孔弱碱性阴离子交换树脂对钼的吸附和洗脱性能.实验结果表明,溶液组成为[Mo]=3.0、[(NH_4)_2SO_4]=100g/dm~3时,树脂对钼的动态吸附容量为244.3mg/m
本文简要叙述超精密加工刀具的特性,正确使用方法及其切削条件。可供从事超精密加工技术人员参考。 This article briefly describes the characteristics of ultra-precisi
对于人教A版《数学》(选修4-4)习题1.3第6题,用配套《教师教学用书》上的方法来做无可厚非。不过,笔者多角度地利用第(1)问的结论,用不同的方法也可以完成第(2)问。下面笔者
我校机械工程一系同汉江机床厂合作研究的科研成果“螺纹智能磨削控制系统的研究”于1992年8月6日至7日在汉江机床厂现场通过了由机 A series of mechanical engineering p
铜管乐器尤其特有的乐器性能,要在M ID I中制作逼真的铜管乐器声部,不仅要考虑乐器本身的性能和音域,还要根据电子乐器的特点做相应的技术处理。 Brass instruments Particu
本文对几种常用的提高极限侧推抗力的方法进行了分析和研究,并提出了一种经济而有效地提高缠绕机架抗侧推能力的方法,供同行们参考。 In this paper, several commonly used
用透射电子显微分析及高分辨技术.研究了(Fe·Cr)_7C_3型碳化物所属的晶系,层错的堆垛类型及孪生轴的方向。研究结果表明:高铬铸铁中(Fe·Cr)_7C_3碳化物属正交晶系并有孪晶
利用金相及断口显微学等方法,系统地分析和研究了造成中高碳钢丝在拉拔过程中脆断的内、外部因素,并指出显微组织不良、夹杂物及折叠等冶金缺陷是导致钢丝脆断的主要原因。
从整体市场来看,中国E-Learning市场导入期尚未完成,尚未有完整的产业链出现,纵向行业市场用户应用及认识水平差别较大.
影响平面高速精磨的工艺因素很多,譬如:平面高速精磨机的机床参数、镜盘的上盘方法、玻璃材料的软硬程度、冷却液、磨盘形式和加工时间等。现就这些因素加以讨论。在试验过